Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 60.0 - 100 MPa | 8700 - 14500 psi | |
Plastcom SLOVALEN PC 59 GF 13 Compounded Polypropylene Homopolymer, 13% Chemically Coupled Glass Fiber FeaturesCompounded homopolymer PP, with the content of 13% chemically coupled glass fiber and modifier of mechanical properties. Increased strength in comparison with unfilled PP. Use in all indus.. |
|||
Injection Pressure | 60.0 - 100 MPa | 8700 - 14500 psi | |
Plastcom SLOVASTER® B GF 30 Polybutylene Terephthalate, 30% Glass Fiber FeaturesPBT for injection moulding, chemically reinforced with 30% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a.. |
|||
Injection Pressure | 60.0 - 100 MPa | 8700 - 14500 psi | |
Plastcom SLOVASTER® B/E GF 30 PBT, 30% glass fibre FeaturesPBT/PET for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and ben.. |
|||
Injection Pressure | 60.0 - 100 MPa | 8700 - 14500 psi | |
Plastcom SLOVASTER® B2 GF 10 PBT, 10% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 10% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Injection Pressure | 60.0 - 80.0 MPa | 8700 - 11600 psi | |
Premix Thermoplastics PRE-ELEC® ESD 5510 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5510 is a static dissipative thermoplastic compound based on polypropylene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 5510 can be injectio.. |
|||
Injection Pressure | 60.0 - 80.0 MPa | 8700 - 11600 psi | |
Premix Thermoplastics PRE-ELEC® PP 1370 PRE-ELEC PP 1370 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Injection Pressure | 60.0 - 100 MPa | 8700 - 14500 psi | |
SABIC M80064 Series High Density Polyethylene for Injection Molding Product Description: M80064 is a high density polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to provide good rigid.. |
|||
Injection Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Celcon® M90UV POM, UV Resistant
(Unverified Data**) Celcon® M90UV is an acetal copolymer developed as a natural UV light stabilized standard flow grade for overall performance in most molding applications. It has been formulated as a natural acetal .. |
|||
Injection Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Hostaform® C 13031 LS POM, UV Resistant
(Unverified Data**) POM copolymerHostaform C 13031 with UV additivesInformation provided by Celanese |
|||
Injection Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Hostaform® C 2521 POM
(Unverified Data**) Chemical abbreviation according to ISO 1043-1: POMStiff-flowing grade for injection molding and extrusionInformation provided by Celanese |
|||
Injection Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Hostaform® C 2521 G POM, Tribological
(Unverified Data**) Chemical abbreviation according to ISO 1043-1: POMStiff-flowing grade for injection molding and extrusion, modified with (R) GUR (PE-UHMW)Information provided by Celanese |
|||
Injection Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Hostaform® C 9021 S1 POM, Tribological
(Unverified Data**) modified with silicon oilInformation provided by Celanese |
|||
Injection Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Hostaform® LW90BSX POM, Tribological
(Unverified Data**) Hostaform® LW90BSX is a specialty low wear grade of acetal copolymer designed for a wide range of tribological applications, including POM/POM pairings. This grade's low wear system includes silic.. |
|||
Injection Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Hostaform® MT24F01 POM, Medical Technology
(Unverified Data**) Hostaform® acetal copolymer grade MT24F01 is a special grade developed for medical industry applications containing low residual monomers and no animal products. Hostaform® MT24F01 is a low level .. |
|||
Injection Pressure | 60.0 - 80.0 MPa | 8700 - 11600 psi | |
Premix Thermoplastics PRE-ELEC® 12-032
(discontinued **) PRE-ELEC 12-032 is a conductive thermoplastic compound based on a polyacetal copolymer with 20% carbon fiber. PRE-ELEC 12-032 exhibits excellent mechanical properties and electrical conductivity. Te.. |
|||
Injection Pressure | 60.0 - 80.0 MPa | 8700 - 11600 psi | |
Premix Thermoplastics PRE-ELEC® 12-033
(discontinued **) PRE-ELEC 12-033 is a conductive thermoplastic compound based on a polyacetal copolymer with 30% carbon fiber. PRE-ELEC 12-033 exhibits excellent mechanical properties and electrical conductivity. Te.. |
|||
Injection Pressure | 60.0 MPa | 8700 psi | |
Covestro Makroblend® UT-408 Polycarbonate + Polyester Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015,.. |
|||
Injection Pressure | 60.0 MPa | 8700 psi | |
Ineos ABS Centrex® 485 ASA+AES Blend
(discontinued **) Key Features:UnfilledLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Profile extrusionSheet extrusionThermoformingInformation provided by Bayer Pol.. |
|||
Injection Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Celcon® M90UV POM, UV Resistant Celcon« M90UV is an acetal copolymer developed as a natural UV light stabilized standard flow grade for overall performance in most molding applications. It has been formulated as a natural acetal .. |
|||
Injection Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Hostaform® C 2521 LS POM, UV Resistant Information provided by Celanese |
|||
Injection Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Hostaform® C 2521 POM, Unfilled Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese |
|||
Injection Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Celcon® M90-34 POM, Unfilled Celcon« M90-34 is a specially formulated injection moldable grade of acetal copolymer for the appliance market targeted at resisting staining while providing a balance of properties.Information pro.. |
|||
Injection Pressure | 60.0 - 90.0 MPa | 8700 - 13100 psi | |
Beijing Chemical Industry KAIFA® HN301-M30 PA6 Resin Mineral filled, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Injection Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Celcon® LW90-S2 POM, Tribological
(Unverified Data**) Celcon® LW90-S2 is a preblended low wear formulation of M90 base polymer containing 2% silicone. This standard low friction, low wear product performs well in many applications including those inv.. |
|||
Injection Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Hostaform® LM140LGZ POM, UV Resistant
(Unverified Data**) Hostaform® acetal copolymer grade LM140LGZ is a laser markable specialty grade of acetal copolymer formulated to provide good flow with a low gloss finish and improved UV resistance.Laser markable,.. |
|||
Injection Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Hostaform® LM90 POM, Specialty
(Unverified Data**) Hostaform® LM90 is a nominal 9 melt flow rate acetal copolymer which is capable of being permanently marked by a laser. Parts molded from Hostaform® LM90 can be laser marked with barcodes, identif.. |
|||
Injection Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Hostaform® M90XAP® POM
(Unverified Data**) Hostaform® acetal copolymer grade M90 XAP® is a low emission version, medium viscosity polymer providing optimum performance in general purpose injection molding primarily for the interior automo.. |
|||
Injection Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Hostaform® XT 20 POM, Impact Modified
(Unverified Data**) Preliminary Data SheetHighly Impact ModifiedInformation provided by Celanese |
|||
Injection Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Hostaform® C 9021 XAP® POM, Unfilled POM copolymerInformation provided by Celanese |
|||
Injection Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Celanese Hostaform® MT12R01 POM, Medical Technology Hostaform« MT12R01 is a special grade developed for medical industry applications containing low residual monomers and no animal products. Hostaform« MT12R01 is a low melt viscosity and improved .. |