Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.580 J/cm @Temperature -30.0 °C |
1.09 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics GELOY CR7020 ASA ASA copolymer. Profile/sheet coextrusion over ABS. Excellent weatherability, good flow/aesthetics and high impact. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP AL003 ABS (Europe-Africa-Middle East) LNP LUBRICOMP* AL003 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
Ineos T50-800 HDPE T50-800 is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and end-use .. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM 2212EPR PEI 20% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA lising. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP WFL369 PBT LNP* Lubricomp* WFL369 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Ret.. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP WX95752L PBT LNP* Lubricomp* WX95752L is a compound based on Polybutylene Terephalate resin. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM 3452 PEI (Asia Pacific) 45% Glass fiber and mineral filled, enhanced flow Polyetherimide (Tg 217C) with enhanced dimensional stability. ECO Conforming, UL94 V0 and 5VA listing in recognized colors. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRILOY U2000A PPA LNP* LUBRILOY* U2000A is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DE0049P PC (Asia Pacific) LNP* Stat-kon* DE0049P is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Exceptional Processing, Flame Retardant. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON EE004 PEI LNP* STAT-KON* EE004 is a compound based on Polyetherimide resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON EE004 PEI (Asia Pacific) LNP* Stat-kon* EE004 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® V8030CS PBT+PET Glass filled Valox with enhanced surface |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON REP349 PA 66 (Asia Pacific) LNP* Stat-kon* REP349 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Izod Impact, Notched | 0.580 J/cm @Temperature 23.0 °C |
1.09 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp GF003 PSU (Asia Pacific) LNP* THERMOCOMP* GF003 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP JF004EXP PES (Asia Pacific) LNP* Thermocomp* JF004EXP is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Easy Molding. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP JF006LXZ PES (Asia Pacific) LNP* Thermocomp* JF006LXZ is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Low Extractible. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP LC008E PEEK LNP* THERMOCOMP* LC008E is a compound based on Polyetheretherketone resin containing 40% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP LC008E PEEK (Asia Pacific) LNP* Thermocomp* LC008E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RF006XXZ PA 66 LNP THERMOCOMP* RF006XXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP UC008H PPA (Asia Pacific) LNP* THERMOCOMP* UC008H is a compound based on Polyphthalamide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched | 0.580 J/cm @Temperature 23.0 °C |
1.09 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp UC008S PPA (Asia Pacific) LNP* Thermocomp* UC008S is a compound based on Polyphthalamide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for.. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL HFM3015P PPE+PS (Asia Pacific) 30% GF/MF filled FR PPE/PS blend |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL HM3020H PPE+PS (Asia Pacific) PPE+PS GF+MF 30% filled, FR V-1, high flow |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DEL339XF PC (Asia Pacific) LNP* Stat-kon* DEL339XF is a compound based on Polycarbonate resin containing PTFE, Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant,.. |
|||
Izod Impact, Notched | 0.580 J/cm @Temperature 23.0 °C |
1.09 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Stat-kon DX96690 PC LNP STAT-KON* DX96690 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the America.. |
|||
Izod Impact, Notched | 0.580 J/cm @Temperature 23.0 °C |
1.09 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Stat-loy W3000 PBT LNP STAT-LOY* W3000 is a compound based on Polybutylene Terephalate resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Americ.. |
|||
Izod Impact, Notched | 0.580 J/cm @Temperature -30.0 °C |
1.09 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX673 PPE+PA Conductive Noryl GTX* resin designed for profile extrusion. This grade can be electrostatic or powder coat painted without the need for a primer. In addition, its high heat capability allows it to .. |
|||
Izod Impact, Notched | 0.580 J/cm @Thickness 3.17 mm |
1.09 ft-lb/in @Thickness 0.125 in |
ASTM Test |
BASF Ultramid® 8202 HS PA6 (Dry) Ultramid 8202 HS is a heat stabilized, low viscosity, general purpose nylon 6 injection molding homopolymer. It possesses the combination of strength and toughness and has excellent chemical and ab.. |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® P106 PBT Polyester A general purpose polyester with low shrinkage and good flow.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON ME006 PP (Asia Pacific) LNP STAT-KON* ME006 is a compound based on Polypropylene resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |