Electrical Properties | Metric | English | Comments |
---|---|---|---|
Static Decay | <= 2.0 sec | <= 2.0 sec | ISO IEC 61340-5-1 |
Premix Thermoplastics PRE-ELEC® ESD 4300 PRE-ELEC ESD 4300 is a static dissipative thermoplastic compound based on PE-LD. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 4300 has been developed for mult.. |
|||
Static Decay | <= 2.0 sec | <= 2.0 sec | FTMS 101B |
Techmer ES Electrablend® PA6 04001 BL Glass/Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Stainless Steel FiberAdditive: LubricatedFeatures: Electromagnetic Shielding (EMI), Lubricated and Radio Frequency Shielding (RFI.. |
|||
Static Decay | <= 2.0 sec | <= 2.0 sec | FTMS 101B |
Techmer ES HiFill® PA6 0254 B2 Barium Sulfate Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific Gravity and AntistaticAdditive: AntistaticInformation provided by TP Composites, Inc. |
|||
Static Decay | <= 2.0 sec | <= 2.0 sec | 12% RH (+5000 V to 50 V); FTMS-101C |
Lubrizol STAT-RITE® S-1107 Static Dissipative TPU Description: Stat-Rite® S-1107 is a static dissipative TPU alloy. Stat-Rite S-1107 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD .. |