Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa EDISTIR SRL800/N High Impact Polystyrene (HIPS)  (discontinued **)

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa EDISTIR SRL800/N High Impact Polystyrene (HIPS)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,G,093-06-07-12 Very high environmental stress cracking resistant (VH ESCR) modified HIPS. It exhibits high toughness and enhanced chemical resistance to oils, fats and chemical agents and in particular to cyclopentane. Suitable for extrusion/ thermoforming and injection molding. Delivered in round pellets, this material can be also supplied in cylindrical pellets as Edistir SRL800 Applications: Designed for inner liners and frames for refrigerators where cyclopentane is used as blowing agent for insulating polyurethane foams.Unfilled. Suitable for Injection Molding, Sheet Extrusion, Blow Molding, Thermoforming. Supplied as pellets. Contains release agent.ISO data. Information provided by EnichemPolimeri Europa now has Enichem's plastics businesses. This grade is no longer in the product line.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Melt Flow 4.2 g/10 min

@Load 5.00 kg,
Temperature 200 °C
4.2 g/10 min

@Load 11.0 lb,
Temperature 392 °F
cm³/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 17.5 MPa
2540 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal
Elongation at Yield 1.7 %
1.7 %
50 mm/min
Tensile Modulus 1.40 GPa
203 ksi
1 mm/min
Charpy Impact Unnotched 16.0 J/cm²
76.1 ft-lb/in²
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
Vicat Softening Point 91.0 °C
196 °F
50°C/hr; 50N
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
Dielectric Constant 2.5

@Frequency 100 Hz
2.5

@Frequency 100 Hz
Dielectric Strength 65.0 kV/mm
1650 kV/in
Dissipation Factor 0.00030

@Frequency 100 Hz
0.00030

@Frequency 100 Hz
Comparative Tracking Index 500 V