Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 78.9 °C | 174 °F | ASTM D-648 |
Plaskolite Optix® CA - 927 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.9 °C | 174 °F | ASTM D648 |
Plaskolite West Optix® CA-990 Impact Modified Acrylic Resin Injection Molding and Extrusion Grade. Excellent surface gloss. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.9 °C | 174 °F | ASTM D-648 |
Plaskolite West Optix® CP - 927 G High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Cycolac® S701SU ABS (Europe-Africa-Middle East) CYCOLAC S701SU is an ABS with improved UV resistance, providing a superior balance of properties. Its wide processing window, excellent flow and good mechanical properties give this material an exce.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C @Thickness 6.40 mm |
174 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics GELOY CR7020 ASA (Asia Pacific) ASA copolymer. Profile/sheet coextrusion over ABS. Excellent weatherability, good flow/aesthetics and high impact. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.9 °C @Thickness 6.35 mm |
174 °F @Thickness 0.250 in |
unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylac® LG35 Low Gloss ABS Acrylonitrile Butadiene Styrene, low gloss ABS.Information provided by Ravago. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | |
Ineos ABS Centrex® 601 ASA+AES Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Profile extrusionSheet extrusionInformation.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.9 °C | 174 °F | ASTM D648 |
I. Stern GPPS-004 General Purpose Crystal Polystyrene Features:High Strength GradeMedium Flow, High ToughnessExcellent ProcessabilityApplicationsInjection MoldingAgency RatingsFDA Title 21 CFR 177.1640UL File E185934Information provided by I. Stern & C.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C @Thickness 6.40 mm |
174 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical HIPS 406AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Office Appliances (Parts of Printer or Copier)CAS: 9003-55-8, 25713-60-4 and 1309-64-4Information provided by LG Chemical |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C @Thickness 6.40 mm |
174 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical LUCEL HI515W POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: Gears, Automobile ClipCAS No. 66455-31-0 and 155123-66-3Information provided by LG Chemical |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C @Thickness 12.7 mm |
174 °F @Thickness 0.500 in |
Unannealed; ASTM D648 |
LG Chemical 501S-S HIPS Self lubricant, Balanced mechanical properties, Good surface appearance with high gloss, Conforming to FDA CFR 177.1640, Excellent processability, Applications include refrigerator food holders, par.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.9 °C @Thickness 6.35 mm |
174 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
Samsung Cheil Industries Starex® VE-0856 (VE-0856U UV) Flame Retardant Grade ABS VE-0856U is the UV-Stabilized Version.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | Unannealed; 104°C (219°F) annealed; ASTM Data |
Styron Magnum™ 2620 ABS, Impact Grade MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | Unannealed; ASTM Data |
Styron Magnum™ 2645 ABS, Impact Grade MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | Unannealed; ASTM Data |
Styron Magnum™ 545 ABS, General Purpose MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | Unannealed; ASTM Data |
Styron Magnum™ 8325 ABS, Sheet Coextrusion Grade MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | Unannealed; 106°C (223°F) annealed; ASTM Data |
Styron Magnum™ 9450P ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics NORYL PVX0800 PPE NORYL* PVX0800 resin is a high flow, V0 = 1.5 mm grade, suitable for a variety of electronics applications. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | ASTM D648 |
Supreme Petrochem SP 554 Flame Retardant Polystyrene Characteristics Very good flow properties Good balance of toughness and rigidity Processing Molding Gas assist molding Applications Large size T.V. Cabinets VCR cabinets Electrical boxes, electr.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.9 °C | 174 °F | ASTM D648 |
Westlake Plastics Corzan® II CPVC Sheet Corzan® II CPVC, manufactured from Corzan G2 resin, was developed for use in the construction of wet benches and other cleanroom equipment for the semiconductor industry. It meets Factory Mutual.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | Conditioned 4 hours @ 70°C (158°F); ASTM D648 |
Eastman Tenite Butyrate 285A2R30016 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 8%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | ISO 75-2 |
Denka TX-400S Transparent Resin Polymer (MS resin) Methyl Methacrylate Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | 0.125";; ASTM D648 |
Diamond Polymers Centrex® 485 Sheet Extrusion Grade Centrex 485 resin is a low-gloss, medium-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.9 °C | 174 °F | |
BCC Products BC 6004 Epoxy Surface Coat BC 6004 is a white thixotropic epoxy surface coat that has the ability to cure and bond to freshly poured wet plaster. This formulated resin compound can be applied with a brush or troweled to a thi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.9 °C | 174 °F | |
Aclo Accucomp SAN SAN900L |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | ASTM D648 |
Adell EQ-14 Homopolymer Polypropylene, 20% Mica Filled Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | ASTM D648 |
Total Lacqrene® 1160(AS) Crystal Polystyrene
(discontinued **) LACQRENE® 1160 is a high resistance, high molecular weight crystal polystyrene mainly for the extrusion industry. It is particularly useful in the production of thick sheet by direct gassing, wher.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | ASTM D648 |
Ineos Nova 5500 High Impact Polystyrene
(discontinued **) Good overall balance of properties, USP Class VIApplications: Audio cassettes and cartridges, Housewares, Toys, Structural foam, Machine housings, Window framesProperties were determined on injectio.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 - 242 °C | 174 - 468 °F | Average value: 212 °C Grade Count:48 |
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | ASTM D648 |
Ineos Nova 5504 High Impact Polystyrene
(discontinued **) Good overall balance of properties, USP Class VIApplications: Audio cassettes and cartridges, Housewares, Toys, Structural foam, Machine housings, Window framesProperties were determined on injectio.. |