Tensile Strength, Yield 17.5 MPa
2540 psi
ISO 527
Polimeri Europa Edistir® PD ICE S 900 High Impact Polystyrene - Very High ESCR
Very high environmental stress cracking resistant (VH ESCR) HIPS.ICE S 900 exhibits high toughness and excellent chemical resistance to oils, fats and chemical agents, and in particular to cyclopent..
Tensile Strength, Yield 17.5 MPa
2540 psi
50 mm/min; ISO 527
Polimeri Europa Edistir ICE S 800/N Polystyrene  (discontinued **)
Very high environmental stress cracking resistant (VH ESCR) modified HIPS. ICE S 800/N exhibits high toughness and excellent chemical resistance to oils, fats and chemical agents and in particular t..
Tensile Strength, Yield 17.5 MPa
2540 psi
50 mm/min
Polimeri Europa EDISTIR SRL800/N High Impact Polystyrene (HIPS)  (discontinued **)
Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,G,093-06-07-12 Very high environmental stress cracking resistant (VH ESCR) modified HIPS. It exhibits high toughness and ..
Tensile Strength, Yield 17.5 MPa

@Thickness 1.91 mm
2540 psi

@Thickness 0.0750 in
Type IV specimen, 2" per minute test speed, compression molded sample; ASTM D 638
NOVA Chemicals Novapol® TR-0535-UI Hexene MDPE Rotational Molding Resin
TR-0530-UI complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. TR-0530-UI is su..
Tensile Strength, Yield 17.5 MPa

@Thickness 1.91 mm
2540 psi

@Thickness 0.0750 in
Type IV specimen, 2" per minute test speed, compression molded sample; ASTM D 638
NOVA Chemicals Novapol® TR-0535-UIG Hexene MDPE Rotational Molding Resin
TR-0530-UIG complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. TR-0530-UIG is ..
Tensile Strength, Yield 17.5 MPa
2540 psi
ASTM D638
Ineos G36-24-149 MDPE with Carbon Black  (discontinued **)
Fortiflex® G36-24-149 is a black medium density polyethylene resin designed for sheet extrusion. This resin has excellent environmental stress crack resistance (ESCR) and ultra violet protection. ..
Tensile Strength, Yield 17.5 - 23.4 MPa
2540 - 3390 psi
Average value: 21.2 MPa Grade Count:7
Overview of materials for High Density Polyethylene (HDPE), Carbon Black Filled
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Carbon Black Filled". Each property range of values reported is minimu..
Tensile Strength, Yield 17.5 MPa
2540 psi
2 in/min (50 mm/min); ASTM D638
Ineos G36-24-150 HDPE
Ineos G36-24-150 is a medium density polyethylene resin designed for geomembrane sheet extrusion. The resin has excellent environmental stress crack resistance (ESCR).Natural resin; some physical p..
Tensile Strength, Yield 17.5 MPa
2540 psi
50 mm/min
Arkema Group Appryl® 7280 Polypropylene - Polyethylene Copolymer
PP/PE copolymer colored directly or during the injection molding process. This grade with a very good impact test at low temperature, has been developed for bumpers applications for the automotive i..
Tensile Strength, Yield 17.5 MPa
2540 psi
ISO 527-2/50
ExxonMobil Exxtral™ H1020H Performance Polyolefin
Product Description: A specialty thermoplastic olefin resin with good flow, cold temperature impact resistance, low CLTE, medium shrinkage and excellent paintability for automotive exterior applicat..
Tensile Strength, Yield 17.5 MPa
2540 psi
150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2
Solvay Engineered Polymers DEXPRO® R225 TPV - High-Impact Polypropylene  (discontinued **)
Description: DEXPRO® R225 is a high-impact polypropylene co-polymer molding compound. Applications: Small exterior trim components. Information provided by Solvay Engineered Polymers. LyondellBasel..
Tensile Strength, Yield 17.5 MPa
2540 psi
150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2
Solvay Engineered Polymers DEXPRO® R210 TPV - High-Impact Polypropylene  (discontinued **)
Description: DEXPRO® R210 is a high-impact polypropylene co-polymer molding compound. Applications: Exterior trimInformation provided by Solvay Engineered Polymers. LyondellBasell acquired Solvay E..
Tensile Strength, Yield 17.5 MPa
2540 psi
150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2
Solvay Engineered Polymers DEXPRO® R116 TPV - High-Impact Polypropylene  (discontinued **)
Description: DEXPRO® R116 is a thermoplastic polyolefin elastomeric. It is unfilled, reactor-grade molding compound. Applications: Exterior trim Information provided by Solvay Engineered Polymers..