Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | IEC 60243 |
Polimeri Europa Edistir ICE R 830D Polystyrene Environmental stress cracking resistant (ESCR) HIPS. ICE PD R 830D combines high impact strength with an improved chemical resistance to oils, fats and chemical agents, such as detergents for both i.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | IEC 60243 |
Polimeri Europa Edistir R 850E Polystyrene Super high impact polystyrene with good heat resistance. Designed for sheet extrusion and thermoforming of deep drawn containers even
diluted with high percentage of GP. Suitable for general injecti.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | IEC 60243 |
Polimeri Europa Edistir RT 441M Polystyrene High impact polystyrene combining high toughness and high stiffness with good flowability for easy processing. Designed for injection moulding of technical parts, housings and covers.
Especially rec.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | IEC 60243 |
Polimeri Europa Edistir SR 550 Polystyrene High impact, easy flow polystyrene with good elasticity at low temperatures.Suitable for injection moulding of large or complex parts with low thickness and high impact strength.
Designation: Thermo.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | IEC 60243 |
Polimeri Europa Edistir RCL 600 Polystyrene
(discontinued **) Special medium impact polystyrene extrusion grade exhibiting very high gloss. This grade should be used where is required an excellent surface finish. It can be directly extruded in foils and sheets.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | |
Polimeri Europa EDISTIR PD RK4514H High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,093-06-07-23 UL94 V-2, polybromodiphenylether (PBBE) free, antimony free, HIPS satisfying at 960°C the glow wire test.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | |
Polimeri Europa EDISTIR PD RK5512G High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,088-06-07-23 UL94 V-2, polybromobiphenylether (PBBE) free, high impact polystyrene with good mechanical and thermal pr.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | |
Polimeri Europa EDISTIR PD RR745E High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,G,088-03-07-12 Environmental stress cracking resistant (ESCR) HIPS. It combines high impact strength with high chemical r.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | |
Polimeri Europa EDISTIR RC3 High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,088-06-07-18 Special high impact, high gloss polystyrene grade. Suitable for injection molding in the appliances sector.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | |
Polimeri Europa EDISTIR RK0414 High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,088-03-04-23 UL94 V-0, polybromobiphenylether (PBBE) free, flame retarded high impact polystyrene with excellent light .. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | |
Polimeri Europa EDISTIR SRL800/N High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,G,093-06-07-12 Very high environmental stress cracking resistant (VH ESCR) modified HIPS. It exhibits high toughness and .. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | IPC-TM-650.2.5.6.2 |
Park Electrochemical Nelco® N8000 Cyanate Ester Epoxy Laminate and Prepreg The Nelco N8000 is a high-Tg cyanate ester laminate and prepreg system that provides superior performance and product integrity and is ideal for board designs with higher layer counts, finer lines a.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | ASTM D149 |
Solvay Specialty Polymers Algoflon® S 131 PTFE (Polytetrafluoroethylene)
(discontinued **) Data provided by the manufacturer.Type IV.G.2 Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric p.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | 200µm film; IEC 60243-1 |
3M Dyneon™ TFM™ 1605 Modified PTFE Powder
(discontinued **) Type III, gr. 2 PTFE. Second-generation PTFE that is a chemically modified to allow new designs and processing methods. Very good free-flowing powder properties.Data provided by Dyneon. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | |
Saint-Gobain CHR® 2042-10 Skived PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | ASTM D149 |
Goodfellow TPX® MX002O Polymethylpentene This grade is highly recommended for injection molding, film and mandrel extrusion; also for fiber extrusion and blow molding.TPX® is semi-crystalline, transparent, very light and - for a polyolefi.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | ASTM D149 |
Goodfellow TPX® RT31XB Injection Molding Grade Polymethylpentene This grade is highly recommended for injection molding; also for film and fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release c.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | ASTM D149 |
Goodfellow TPX® DX845 Extrusion Grade Polymethylpentene This grade is highly recommended for film extrusion; also for injection molding, fiber extrusion and blow molding.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensiv.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | ASTM D149 |
Goodfellow TPX® RT31 Injection Molding Grade Polymethylpentene This grade is highly recommended for injection molding; also for film and fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release c.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | ASTM D149 |
Solvay Specialty Polymers Algoflon® F2 PTFE (Polytetrafluoroethylene)
(discontinued **) Data provided by the manufacturer.Type II Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric prope.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | ASTM D149 |
Solvay Specialty Polymers Algoflon® A.15 PTFE (Polytetrafluoroethylene)
(discontinued **) Data provided by the manufacturer.Type IV.G.1 Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric p.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | |
Polimeri Europa EDISTIR PD RK6223N High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,083-12-07-23 Halogen and Antimony free, medium impact polystyrene. This grade complies at 2 mm with IEC 65-20-2 and BSI.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | |
Polimeri Europa EDISTIR SRL550 High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,E,083-12-07-18 High impact, easy flow polystyrene with good elasticity at low temperatures. Used for sheet extrusion and .. |
|||
Dielectric Strength | 65.0 - 146 kV/mm | 1650 - 3710 kV/in | Average value: 75.1 kV/mm Grade Count:8 |
Overview of materials for Polymethylpentene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polymethylpentene, Molded". Each property range of values reported is minimum and maximum values of appr.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | ASTM D149 |
Mitsui TPX® DX820 Methylpentene Copolymer TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |
|||
Dielectric Strength | 65.0 kV/mm | 1650 kV/in | ASTM D149 |
Mitsui TPX® MX004 Methylpentene Copolymer TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |