Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 79.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
ASTM D648
Plaskolite Optix® CA-927 Impact Modified Acrylic Resin
Injection Molding Grade Pellets. Better impact strength than CA-924. Excellent surface gloss, optical clarity, and practical toughness.
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
SABIC Innovative Plastics Cycolac® S701SU ABS (Europe-Africa-Middle East)
CYCOLAC S701SU is an ABS with improved UV resistance, providing a superior balance of properties. Its wide processing window, excellent flow and good mechanical properties give this material an exce..
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
Polimeri Europa EDISTIR N1461 Polystyrene  (discontinued **)
Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,M,085-03 High molecular weight general purpose polystyrene with good mechanical strength. Well suitable for injection mold..
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C

@Thickness 6.40 mm
174 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics GELOY CR7520 ASA
General purpose ASA. Excellent weatherability, good flow/aesthetics and high impact. Rated F2 by UL.
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C

@Thickness 3.17 mm
174 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Ineos ABS Centrex® 401 AES Extrusion  (discontinued **)
Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
ASTM Data
BASF Capron® 8200CQ Blend Nylon 6 (Dry)  (discontinued **)
Capron 8200CQ Blend is a medium viscosity, nylon 6 injection molding homopolymer possessing the combination of strength, stiffness and toughness properties as well as chemical and abrasion resistanc..
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C

@Thickness 6.40 mm
174 °F

@Thickness 0.252 in
ASTM D648
Kingfa FRHIPS-301 Flame Retardant Polystyrene
Features:UL 94 V-1 @ 2.0 & 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingElectrica..
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C

@Thickness 6.40 mm
174 °F

@Thickness 0.252 in
Unannealed; ASTM D648
LG Chemical ALPHALAC SG960 HIPS
Description: Injection Molding, General Purpose, Good ProcessabilityApplication: Washer Cover, Air-conditioner Panel, Refrigerator PartsCAS No. 9003-55-8Information provided by LG Chemical
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C

@Thickness 6.40 mm
174 °F

@Thickness 0.252 in
Unannealed; ASTM D648
LG Chemical LI931 Extrusion ASA
Description: Low Gloss, Extrusion Application: Industrial Materials (Window Profile, Tile Etc)CAS: 26299-47-8 & 9003-54-7Information provided by LG Chemical
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
ISO 75-2
Kureha KF Polymer 1000 PVDF Homopolymer
KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p..
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
Annealed; ASTM D648
Spartech Royalite R61M Low Smoke Resin
Data provided by the manufacturer. Formulated to meet smoke and fire specifications recommended by the FTA, this is ideally suited for mass transit applications such as seat backs, overhead storage..
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C

@Thickness 6.40 mm
174 °F

@Thickness 0.252 in
ASTM D648
Samsung Cheil Industries Starex® NH-1904 HIPS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C

@Thickness 3.20 mm
174 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP RZ006S PA 66
LNP* THERMOCOMP* RZ006S is a compound based on Nylon 66 resin containing 30% Milled Glass. Added feature of this material is: Heat Stabilized.
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
Unannealed; ASTM Data
Styron Magnumâ„¢ 2645 ABS, Impact Grade
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
Unannealed; ASTM Data
Styron Magnumâ„¢ 342EZ ABS, Medium Impact
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
Unannealed; ASTM Data
Styron Magnumâ„¢ 8325 ABS, Sheet Coextrusion Grade
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP THERMOCOMP AB002 ABS
LNP* THERMOCOMP* AB002 is a compound based on ABS resin containing 10% Glass Bead.
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
ASTM D648
Supreme Petrochem SC 202LV General Purpose Polystyrene
CharacteristicsHigh strength grade Excellent process ability High ClarityProcessing Injection moldingApplications Ball pen barrels, geometrical instruments etc. Suitable for fast cycling products ..
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
ASTM D648
Supreme Petrochem SP 554 Flame Retardant Polystyrene
Characteristics Very good flow properties Good balance of toughness and rigidity Processing Molding Gas assist molding Applications Large size T.V. Cabinets VCR cabinets Electrical boxes, electr..
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
ISO 75
Polyram RamShine PV527 Acrylonitrile Butadiene Styrene, Flame Retardant
Flame retardant ABS for injection molding applications.Information provided by Polyram.
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
ASTM D648
Eastman Tenite 485E3720008 Cellulose Acetate Butyrate, Clear, Trsp
Applications:Toys/Sporting goodsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties including toughness, hardness, strength, surface gloss, clarity,..
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
Conditioned 4 hours @ 70°C (158°F); ASTM D648
Eastman Tenite Butyrate 285A2R30016 Natural, Trsp Cellulose Acetate Butyrate
Plasticizer 8%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
unannealed; ISO 75
Chi Mei Polyrex® PH-888G Polystyrene - High gloss
High impact; high gloss
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
ISO 75-2
Denka TX-400S Transparent Resin Polymer (MS resin) Methyl Methacrylate Styrene
"TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a..
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
ASTM D648
Ashley Polymers Ashlene® 526LD Nylon 66
Modified for toughness at low temperatures, injection molding grade.Data provided by the manufacturer
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
ASTM D648
A. Schulman ComAlloy Lubrilon® 602 Nylon 6/6, Molybdenum Disulfide Filled, Flow Enhanced
Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma..
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
ASTM D648
A. Schulman ComAlloy Voloy® 431 Glass/Mineral Reinforced, PET Alloy, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.40% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
ASTM D648
Ineos Nova 5500 High Impact Polystyrene  (discontinued **)
Good overall balance of properties, USP Class VIApplications: Audio cassettes and cartridges, Housewares, Toys, Structural foam, Machine housings, Window framesProperties were determined on injectio..
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
Unannealed; 104°C (219°F) annealed; ASTM Data
Styron Magnum™ 9020 ABS, High Gloss
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM AB..
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
ASTM D648
Ineos Nova 5504 High Impact Polystyrene  (discontinued **)
Good overall balance of properties, USP Class VIApplications: Audio cassettes and cartridges, Housewares, Toys, Structural foam, Machine housings, Window framesProperties were determined on injectio..