Plenco 1530 Polyester, Briquette, Transfer Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass and Mineral Filled BMC
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 1530 Polyester, Briquette, Transfer Molded.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PLENCO 01530 is a glass and mineral reinforced pelletized polyester molding compound, offering improved mechanical strength properties along with excellent electrical properties and dimensional stability. UL recognized under component file E40654. 01530 is available in black, grey, or blue color.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.880 g/cc
0.0318 lb/in³
ASTM D1895
Density 1.99 g/cc
0.0719 lb/in³
ASTM D792
Water Absorption 0.138 %
0.138 %
ASTM D570
Linear Mold Shrinkage 0.00116 cm/cm
0.00116 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 76
76
ASTM D785
Tensile Strength, Ultimate 83.0 MPa
12000 psi
ASTM D638
Elongation at Break 0.62 %
0.62 %
ASTM D638
Tensile Modulus 18.2 GPa
2640 ksi
ASTM D638
Flexural Strength 140 MPa
20300 psi
ASTM D790
Flexural Modulus 18.3 GPa
2650 ksi
ASTM D790
Compressive Strength 202 MPa
29300 psi
ASTM D695
Poissons Ratio 0.32
0.32
ASTM D638
Shear Modulus 6.89 GPa
999 ksi
Calculated
Izod Impact, Notched 0.410 J/cm
0.768 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.380 J/cm²
1.81 ft-lb/in²
ASTM D256
Impact 179
179
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 54.0 µm/m-°C

@Temperature 40.0 - 130 °C
30.0 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Maximum Service Temperature, Air 223 °C
433 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 264 °C
507 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Oxygen Index 26 %
26 %
ASTM D2863
Shrinkage 0.0044 %
0.0044 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 3.10e+15 ohm-cm
3.10e+15 ohm-cm
ASTM D247
Dielectric Constant 4.5
4.5
ASTM D150
Dielectric Strength 11.8 kV/mm
300 kV/in
Step by Step; ASTM D149
14.8 kV/mm
376 kV/in
Short Time; ASTM D149
Dielectric Breakdown 23000 V
23000 V
1hr 120C; ASTM D149
Dissipation Factor 0.0142
0.0142
ASTM D150
Arc Resistance 191 sec
191 sec
ASTM D495
Comparative Tracking Index 600 V
600 V
ASTM D3638