Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 18.2 GPa | 2640 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP VERTON UX03320 PPA LNP* VERTON* UX03320 is a compound based on Polyphthalamide resin containing proprietary fillers. Added feature of this grade is: Structural. |
|||
Tensile Modulus | 18.2 GPa | 2640 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP VERTON UX03320 PPA (Europe-Africa-Middle East) VERTON* UX03320 is a compound based on Polyphthalamide resin containing Long Glass. |
|||
Tensile Modulus | 18.2 GPa | 2640 ksi | ASTM D638 |
Plenco 1530 Polyester, Briquette, Transfer Molded PLENCO 01530 is a glass and mineral reinforced pelletized polyester molding compound, offering improved mechanical strength properties along with excellent electrical properties and dimensional stab.. |
|||
Tensile Modulus | 18.2 GPa | 2640 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP VERTON UX03320 PPA (Asia Pacific) VERTON* UX03320 is a compound based on Polyphthalamide resin containing Long Glass. |