Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.99 g/cc | 0.0719 lb/in³ | |
Pyrotek Pyrocast AR-S Castable Refractory Pyrocast AR-S is a low cement, fused silica, castable refractory which exhibits excellent resistance to thermal shock. It is inert to liquid aluminum and its alloys. It is a high strength material.. |
|||
Density | 1.99 g/cc | 0.0719 lb/in³ | 50% Resin Content; Internal Method |
Park Electrochemical Nelco® N4000-29 BC® Buried Capacitance™ Multifunctional Epoxy The Nelco N4000-29 is a lead-free, low-CTE, high Tg multifunctional epoxy substrate which has been designed for use in standard multilayer PWB designs and today’s toughest, high-performance, lead-f.. |
|||
Density | 1.99 g/cc | 0.0719 lb/in³ | |
ITW Devcon Metal Repair Wear Resistant Epoxy (WR-2), Dark Grey Information provided by ITW Devcon |
|||
Density | 1.99 g/cc | 0.0719 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Ryton® R-7-120BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-120NA and R-7-120BL glass fiber and mineral filled polyphenylene sulfide compounds provide good strength and low maintenance molding using conventional molding equipment.Features: Good.. |
|||
Density | 1.99 g/cc | 0.0719 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Ryton® R-7-120NA Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-120NA and R-7-120BL glass fiber and mineral filled polyphenylene sulfide compounds provide good strength and low maintenance molding using conventional molding equipment.Features: Good.. |
|||
Density | 1.99 g/cc | 0.0719 lb/in³ | ASTM D792 |
Plenco 1530 Polyester, Briquette, Injection Molded PLENCO 01530 is a glass and mineral reinforced pelletized polyester molding compound, offering improved mechanical strength properties along with excellent electrical properties and dimensional stab.. |
|||
Density | 1.99 g/cc | 0.0719 lb/in³ | ASTM D792 |
Plenco 1530 Polyester, Briquette, Transfer Molded PLENCO 01530 is a glass and mineral reinforced pelletized polyester molding compound, offering improved mechanical strength properties along with excellent electrical properties and dimensional stab.. |
|||
Density | 1.99 g/cc | 0.0719 lb/in³ | ISO 1183 |
Vyncolit BXE650 Inorganic Filled Phenolic Molding Compound Novolac resin based, inorganic filled. Excellent isotropic properties and superior dimensional stability. High mechanical properties even at elevated temperaturesInformation provided by Sumitomo Bak.. |
|||
Density | 1.99 g/cc | 0.0719 lb/in³ | 50% Resin Content; Internal Method |
Park Electrochemical Nelco® N4000-29 Multifunctional Epoxy The Nelco N4000-29 is an advanced, lead-free, low-CTE, high Tg (185º C by DSC) multifunctional epoxy dielectric substrate. This material has been designed for use not only in standard multilayer PW.. |
|||
Density | 1.99 g/cc | 0.0719 lb/in³ | As Molded |
Vyncolit INSUL-PLATE™ X-28057-2HT Hole-Fill Powder For Printed Circuit Boards Vyncolit INSUL-PLATE™ Hole-Fill material delivers true reliability and superior performance. This material, in powder form, is specifically suited for Hole-Fill use in glass epoxy, multi-layer and .. |
|||
Density | 1.99 g/cc | 0.0719 lb/in³ | |
LATI Laticonther 57 CPG/550 PPA, Glass Fiber Reinforced High thermal conductivity product based on Semi-aromatic polyamide (PPA). Special filler. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformat.. |
|||
Density | 1.99 g/cc | 0.0719 lb/in³ | ASTM D792 |
Sumitomo Bakelite North America Epiall® 1914A Short Glass Fiber Reinforced Epoxy Epiall 1914A is a short fiberglass reinforced epoxy molding compound, with excellent dimensional stability, good strength properties and good electrical insulation properties.Information provided by.. |