Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 202 MPa | 29300 psi | ASTM D695 |
Greene Tweed WR™ 300 PEEK, Carbon Filled WR®300 is a carbon-fiber reinforced compression molded PEEK often selected by pump manufacturers and users for pump bushings and case or impeller wear rings. Maximum service life is achieved in .. |
|||
Compressive Strength | 202 MPa | 29300 psi | ASTM D695 |
Plenco 1530 Polyester, Briquette, Transfer Molded PLENCO 01530 is a glass and mineral reinforced pelletized polyester molding compound, offering improved mechanical strength properties along with excellent electrical properties and dimensional stab.. |
|||
Compressive Strength | 202 MPa | 29300 psi | ASTM D695 |
Plenco 2535 Phenolic, Granular, Injection Molded PLENCO 02535 is a general purpose, organic filled phenolic molding compound offering optimized cure characteristics and excellent electrical properties. Type ASTM 5948 CFG, and UL recognized under c.. |