Mechanical Properties Metric English Comments
Izod Impact, Notched 0.410 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
0.768 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion L4536 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Izod Impact, Notched 0.410 J/cm
0.768 ft-lb/in
ASTM D256
Proto3000 Duraform® GF Selective Laser Sintering (SLS®) Prototyping Polymer
Description: Glass-filled polyamide (nylon) material for real-world physical testing and functional useFeatures:Excellent mechanical stiffnessElevated temperature resistanceDimensionally stableEasy-..
Izod Impact, Notched 0.410 J/cm
0.768 ft-lb/in
ASTM D256
North Wood Plastics PS with 20% Wood Fiber
Data provided by North Wood Plastics, Inc.
Izod Impact, Notched 0.410 J/cm

@Thickness 3.17 mm
0.768 ft-lb/in

@Thickness 0.125 in
ASTM D256
Chevron Phillips K-Resin® KR99HG Styrene-Butadiene Copolymer, Injection Molding Grade  (discontinued **)
Styrene-Butadiene CopolymerCustomer Benefits: This SBC is easily processed by injection molding. Molded parts provide excellent part detail on fast production cycles. Molded parts have excellent c..
Izod Impact, Notched 0.410 J/cm
0.768 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP KL003LH Acetal
LNP* LUBRICOMP* KL003LH is an Acetal based compound containing 15% PTFE. Added features of this grade include: Low Extractable, Healthcare, Wear Resistant.
Izod Impact, Notched 0.410 J/cm
0.768 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP MX06404 PP
LNP LUBRICOMP* MX06404 is a compound based on Polypropylene resin containing 20% Glass Fiber and 15% PTFE. Added features of this material include: Heat Stabilized, Low Extractable, Wear Resistant...
Izod Impact, Notched 0.410 J/cm
0.768 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP RBL36L PA 66
LNP* LUBRICOMP* RBL36L is a compound based on Nylon 66 containing 30% Glass Bead, 15% PTFE. Added features s of this grade are: Low Extractable, Wear Resistant.
Izod Impact, Notched 0.410 J/cm

@Temperature 23.0 °C
0.768 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Stat-kon OEL36A PPS
LNP* Stat-Kon* OEL36A is a compound based on Polyphenylene Sulfide resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This ..
Izod Impact, Notched 0.410 J/cm
0.768 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP STAT-KON OEL36A PPS - BRANCHED
LNP* STAT-KON* OEL36A is a compound based on PPS - Branched resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive.
Izod Impact, Notched 0.410 J/cm

@Temperature 23.0 °C
0.768 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Thermocomp JF003L PES
LNP* Thermocomp* JF003L is a compound based on Polyethersulfone (PES) containing Glass Fiber. Characteristics of this grade are Low Extractable.This data was supplied by SABIC-IP for the Americas r..
Izod Impact, Notched 0.410 J/cm

@Temperature 23.0 °C
0.768 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Valox® SLWM2105 PBT+PC (Asia Pacific)
Anti-static PBT/PC blend, mineral 5% filled productThis data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched 0.410 J/cm
0.768 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP STAT-LOY SLWM2105 PBT+PC (Asia Pacific)
Anti-static PBT/PC blend, mineral 5% filled product
Izod Impact, Notched 0.410 J/cm
0.768 ft-lb/in
ASTM D256
Plenco 1530 Polyester, Briquette, Transfer Molded
PLENCO 01530 is a glass and mineral reinforced pelletized polyester molding compound, offering improved mechanical strength properties along with excellent electrical properties and dimensional stab..
Izod Impact, Notched 0.410 J/cm
0.768 ft-lb/in
ASTM D256
Plenco 1586 Polyester, Pellet, Injection Molded
PLENCO 01586 is a glass and mineral reinforced pelletized polyester molding compound offering excellent heat resistance and mechanical strength properties. This product is typically used for injecti..
Izod Impact, Notched 0.410 J/cm
0.768 ft-lb/in
ASTM D256
Plenco 6990 Phenolic, Briquette, Compression Molded
PLENCO 06990 is a glass and mineral filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco.
Izod Impact, Notched 0.410 J/cm

@Thickness 3.17 mm
0.768 ft-lb/in

@Thickness 0.125 in
ASTM D256
Chevron Phillips K-Resin® KR03 Styrene-Butadiene Copolymer, Sheet Grade
Styrene-Butadiene CopolymerCustomer Benefits: This SBC is easily processed by injection molding or sheet extrusion and molded parts give excellent part detail on fast production cycles. It can be t..
Izod Impact, Notched 0.410 J/cm

@Thickness 3.17 mm
0.768 ft-lb/in

@Thickness 0.125 in
ASTM D256
Chevron Phillips K-Resin® KR03NW Styrene-Butadiene Copolymer, Sheet Grade
Styrene-Butadiene Copolymer. No wax (NW) form of K-Resin® KR03 to facilitate printing.Customer Benefits: This SBC is easily processed by injection molding or sheet extrusion and molded parts give ..
Izod Impact, Notched 0.410 J/cm

@Thickness 3.17 mm
0.768 ft-lb/in

@Thickness 0.125 in
ASTM D256
Chevron Phillips K-Resin® KR05 Styrene-Butadiene Copolymer, Sheet and Blow Mold Grade
Styrene-Butadiene CopolymerCustomer Benefits: This SBC is easily processed on blow molding or extrusion and thermoforming equipment. Finished products have excellent clarity, good toughness, good s..
Izod Impact, Notched 0.410 J/cm

@Thickness 3.17 mm
0.768 ft-lb/in

@Thickness 0.125 in
ASTM D256
Chevron Phillips K-Resin® KR05NW Styrene-Butadiene Copolymer, Sheet and Blow Mold Grade
Styrene-Butadiene Copolymer. No wax (NW) form of K-Resin® KR05 to facilitate printing.Customer Benefits: This SBC is easily processed on blow molding or extrusion and thermoforming equipment. Fin..
Izod Impact, Notched 0.410 J/cm

@Temperature 23.0 °C
0.768 ft-lb/in

@Temperature 73.4 °F
ASTM D256
3D Systems DuraForm® GF Glass Filled Nylon
For use with all selective laser sintering (SLS®) systems.ApplicationsHousings and enclosuresConsumer sporting goodsAppropriate for low- to mid-volume rapid manufacturingParts requiring machining o..
Izod Impact, Notched 0.410 J/cm
0.768 ft-lb/in
ASTM-D256
Braskem H 611 HOMO Polypropylene Homopolymer
H 611 is a low melt flow rate homopolymer that was specially designed for exposure to solar light. This product exhibits good processability and high melt resistance. It is designed for raffia extru..
Izod Impact, Notched 0.410 J/cm

@Temperature -30.0 °C
0.768 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics NORYL RN0612 PPE+HIPS (Europe-Africa-Middle East)
Noryl RN0612 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen..
Izod Impact, Notched 0.410 J/cm
0.768 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP STAT-KON ME006 PP
LNP STAT-KON* ME006 is a compound based on Polypropylene resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.