Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | 23000 V | 23000 V | 1hr 120C; ASTM D149 |
Plenco 08112 Polyester BMC, Compression Molded PLENCO 08112 is a renumber of PlasGlas 10112. PLENCO 08112 is a general purpose polyester bulk molding compound that is characterized by adding utility to a number of applications. Because of its co.. |
|||
Dielectric Breakdown | 23000 V | 23000 V | 1hr 120C; ASTM D149 |
Plenco 08235 Polyester BMC, Compression Molded PLENCO 08235 is a renumber of PlasGlas 20315. PLENCO 08235 is a 15% glass-filled polyester bulk molding compound characterized as a flame-retardant, medium strength electrical grade. It is suitable .. |
|||
Dielectric Breakdown | 23000 V | 23000 V | 1hr 120C; ASTM D149 |
Plenco 1510 Polyester, Pellet, Injection Molded PLENCO 01510 is a mineral filled, pelletized polyester molding compound, which offers an excellent combination of electrical properties and dimensional stability. UL recognized under component file .. |
|||
Dielectric Breakdown | 23000 V | 23000 V | 1hr 120C; ASTM D149 |
Plenco 1530 Polyester, Briquette, Injection Molded PLENCO 01530 is a glass and mineral reinforced pelletized polyester molding compound, offering improved mechanical strength properties along with excellent electrical properties and dimensional stab.. |
|||
Dielectric Breakdown | 23000 V | 23000 V | 1hr 120C; ASTM D149 |
Plenco 1530 Polyester, Briquette, Transfer Molded PLENCO 01530 is a glass and mineral reinforced pelletized polyester molding compound, offering improved mechanical strength properties along with excellent electrical properties and dimensional stab.. |
|||
Dielectric Breakdown | 23000 V | 23000 V | 1hr 120C; ASTM D149 |
Plenco 1586 Polyester, Pellet, Injection Molded PLENCO 01586 is a glass and mineral reinforced pelletized polyester molding compound offering excellent heat resistance and mechanical strength properties. This product is typically used for injecti.. |
|||
Dielectric Breakdown | 23000 V @Temperature 121 °C, Time 3600 sec |
23000 V @Temperature 250 °F, Time 1.00 hour |
ASTM D149 |
Plenco 1586 Polyester, Pellet, Transfer Molded PLENCO 01586 is a glass and mineral reinforced pelletized polyester molding compound offering excellent heat resistance and mechanical strength properties. This product is typically used for injecti.. |
|||
Dielectric Breakdown | 23000 V | 23000 V | 1hr 120C; ASTM D149 |
Plenco 1510 Polyester, Granular, Transfer Molded PLENCO 01510 is a mineral filled, pelletized polyester molding compound, which offers an excellent combination of electrical properties and dimensional stability. UL recognized under component file .. |