Polymer Property : Volume Resistivity = 3.10e+15 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 3.10e+15 ohm-cm
3.10e+15 ohm-cm
ASTM D247
Plenco 1530 Polyester, Briquette, Transfer Molded
PLENCO 01530 is a glass and mineral reinforced pelletized polyester molding compound, offering improved mechanical strength properties along with excellent electrical properties and dimensional stab..
Volume Resistivity 3.10e+15 ohm-cm
3.10e+15 ohm-cm
Loctite® 3532 High viscosity Dam Encapsulant
COB/DCA Encapsulants are essential to the reliability of flip chip assemblies because they minimize the thermal mismatch between the flip chip and substrate.Loctite® Underfills and Encapsulants imp..
Volume Resistivity 3.10e+15 ohm-cm
3.10e+15 ohm-cm
Dow Corning SILASTIC® 9251/45 A&B KIT
45 Durometer, 2-part, 1 to 1 mix, off-white, Fabric Coating grade, Liquid Silicone Rubber.Information provided by Dow Corning