Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00116 cm/cm | 0.00116 in/in | ASTM D955 |
Plenco 1530 Polyester, Briquette, Transfer Molded PLENCO 01530 is a glass and mineral reinforced pelletized polyester molding compound, offering improved mechanical strength properties along with excellent electrical properties and dimensional stab.. |
|||
Linear Mold Shrinkage | 0.00116 cm/cm | 0.00116 in/in | ASTM D955 |
Plenco 6500 Phenolic, Briquette, Transfer Molded PLENCO 06500 is a glass reinforced phenolic molding compound offering improved strength, dimensional stability, and excellent electrical properties. UL recognized under component file E40654. 06500 .. |