Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PlastxWorld CEVIAN® B5524 20% GF PBT/ABS Alloy

Category Polymer , Thermoplastic , ABS Polymer , ABS/Polyester Alloy + GF , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer PlastxWorld, Inc.
Trade Name CEVIAN®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastxWorld CEVIAN® B5524 20% GF PBT/ABS Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass fiber reinforced and flame retarded PBT/ABS alloy.Information provided by PlastxWorld Inc.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0025 - 0.0045 cm/cm
0.0025 - 0.0045 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 95.8 MPa
13900 psi
ASTM 638
Elongation at Break 2.4 %
2.4 %
ASTM D638
Flexural Yield Strength 132 MPa
19200 psi
ASTM D790
Flexural Modulus 6.47 GPa
939 ksi
ASTM D790
Izod Impact, Notched 0.694 J/cm

@Thickness 3.17 mm
1.30 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 200 °C
392 °F
0.25 inch; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 125 °C
257 °F
0.25 inch; ASTM D648
UL RTI, Electrical 140 °C
284 °F
UL746B
UL RTI, Mechanical with Impact 95.0 °C
203 °F
UL746B
UL RTI, Mechanical without Impact 130 °C
266 °F
UL746B
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Users viewing this material also viewed the following: