Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 132 MPa | 19200 psi | DIN 53455; ASTM D790 |
Kolon SPESIN® KP213G15HI Multi Reinforced PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Flexural Yield Strength | 132 MPa | 19200 psi | DIN 53455; ASTM D790 |
Kolon KOPA® KN3322VO Flame Retardant Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Flexural Yield Strength | 132 MPa | 19200 psi | ASTM D790 |
Samyang Tribit® 1500GN15 Polybutylene Terephthalate, 15% Glass Reinforced, Flame Retardant Characteristics:G/F reinforcedFlame retardantHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A.. |
|||
Flexural Yield Strength | 132 MPa | 19200 psi | ASTM D790 |
PlastxWorld CEVIAN® B5524 20% GF PBT/ABS Alloy Glass fiber reinforced and flame retarded PBT/ABS alloy.Information provided by PlastxWorld Inc. |
|||
Flexural Yield Strength | 132 MPa | 19200 psi | ASTM D790 |
Cheng Yu Plastic N6CV3 Flame Retardant Nylon 6, 30% Mineral Reinforced |
|||
Flexural Yield Strength | 132 MPa | 19200 psi | ASTM D790 |
Cheng Yu Plastic NG1100S Nylon 66, 10% Glass Fiber Reinforced |
|||
Flexural Yield Strength | 132 MPa | 19200 psi | ASTM D790 |
Cheng Yu Plastic FR200GV10 Flame Retardant Nylon 66, 10% Glass Fiber |