Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.694 J/cm @Temperature 23.0 °C |
1.30 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products FT4600-152 Thermoplastic Polyolefin, UV Stabilized, JA6A Black Applications: Scuff platesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 0.694 J/cm @Temperature 23.0 °C |
1.30 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products GC20P100-177UV 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, (Chrysler HS5) Gray Applications: Air Ducts - distributionBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 0.694 J/cm | 1.30 ft-lb/in | ASTM D256 |
Omni Plastics OmniTech™ PA6/6 GR23 OBHS Optical Bright Glass Reinforced OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and .. |
|||
Izod Impact, Notched | 0.694 J/cm @Temperature 23.0 °C |
1.30 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Ovation Polymers Nemcon™ E PC 08CF Polycarbonate Nemcon E-series products are designed for use in ESDA electronic assembly environments where strict control of ESD and cleanliness are critical. Nemcon E PC 08CF is a carbon fiber-reinforced polyca.. |
|||
Izod Impact, Notched | 0.694 J/cm @Temperature 23.0 °C |
1.30 ft-lb/in @Temperature 73.4 °F |
Method A; ASTM D256 |
Phillips 66 COPYLENE® CR120CL Polypropylene, Random Copolymer, Clarified, Lubricated Random clarified copolymer specially formulated to achieve high clarity and excellent color and color stability with excellent mold release properties. Applications: Injection molding applications s.. |
|||
Izod Impact, Notched | 0.694 J/cm | 1.30 ft-lb/in | Method A; ASTM D256 |
Phillips 66 COPYLENE® CR350CL-02 Polypropylene, Random Copolymer, Clarified CR350CL-02 is a clarified, random copolymer specially designed for clear injection molding applications and is formulated with lube for excellent mold release.Potential Applications: Injection moldi.. |
|||
Izod Impact, Notched | 0.694 - 2.67 J/cm | 1.30 - 5.00 ft-lb/in | Average value: 1.16 J/cm Grade Count:9 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
Izod Impact, Notched | 0.694 J/cm @Temperature 22.8 °C |
1.30 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC/ABS-G30 General Purpose PC/ABS Alloy, 30% Glass Filled PC/ABS Alloy, General Purpose, 30% Glass FilledProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provi.. |
|||
Izod Impact, Notched | 0.694 J/cm @Thickness 3.17 mm |
1.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrablend® PA12 CB Availability: North AmericaForms: PelletsAdditive: Carbon BlackFeatures: ConductiveAppearance: BlackTPCI# 9874105Information provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.694 J/cm | 1.30 ft-lb/in | ASTM D256 |
Techmer ES Electrafil® M-1322 PA66 / PA6 |
|||
Izod Impact, Notched | 0.694 J/cm @Temperature 22.8 °C |
1.30 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Spartech PP5420 Glass Fiber Reinforced Homopolymer Provides the maximum strength and heat resistance among polypropylene compounds. Physical properties can approach those of more expensive engineering resins.Information provided by Spartech |
|||
Izod Impact, Notched | 0.694 J/cm @Thickness 3.17 mm |
1.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PET GF/M35 35% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 35% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.694 J/cm @Thickness 3.17 mm |
1.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® PA4/6 CF30 TL15 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance and Low FrictionInformation p.. |
|||
Izod Impact, Notched | 0.694 J/cm | 1.30 ft-lb/in | ASTM D256 |
Teknor Apex Sinvicomp SRF 2703 Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: Good Weather Resistance; Good Impact Resistance Uses: Fittings Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Izod Impact, Notched | 0.694 J/cm @Temperature 22.8 °C |
1.30 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant 6618G15 HSL UV Black Nylon 66, 15% Glass Fiber, Impact Modified, UV and Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 0.694 J/cm @Temperature 22.8 °C |
1.30 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Ensinger TECASON™ S Polysulfone (PSU) TECASON™ S is a transparent engineering plastic known for its chemical resistance, rigidity, high-temperature performance, and its ability to operate in an autoclave environment. TECASON™ S is FD.. |
|||
Izod Impact, Notched | 0.694 J/cm @Thickness 3.17 mm |
1.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PlastxWorld CEVIAN® B2504 20% GF PBT/ABS Alloy Glass fiber reinforced PBT/ABS alloy.Information provided by PlastxWorld Inc. |
|||
Izod Impact, Notched | 0.694 J/cm | 1.30 ft-lb/in | ASTM Data |
Styron Magnum™ 9100 MFD ABS Data provided by Dow Chemical.This product line was spun off from Dow Chemical to Styron in 2010. |
|||
Izod Impact, Notched | 0.694 J/cm | 1.30 ft-lb/in | ASTM D256 |
Amco PRIMATOP HDPE 055952 Injection Molding Polyethylene HDPE 055952 features maximum toughness, good top loading capability, and high surface gloss. Applications include pails and beverage crates.Former A-Top Polymers product; part of Amco product line s.. |
|||
Izod Impact, Notched | 0.694 J/cm @Temperature -30.0 °C |
1.30 ft-lb/in @Temperature -22.0 °F |
PB; ASTM D256 |
Solvay Engineered Polymers SEQUEL® E2200 TPO
(discontinued **) Description: SEQUEL® E2200 thermoplastic olefinic elastomer (TPO) is designed for thermoformed exterior and interior applications that require low-temperature toughness and high rigidity. This pro.. |