Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Electrical | 140 °C @Thickness 0.750 mm |
284 °F @Thickness 0.0295 in |
UL 746B |
DuPont Performance Polymers Crastin® SK645FR BK851 PBT
(Unverified Data**) Crastin® SK645FR BK851 is a flame retardant , 30% glass reinforced black polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.75mm.Information provided by DuPont Performance P.. |
|||
UL RTI, Electrical | 140 °C @Thickness 0.860 mm |
284 °F @Thickness 0.0339 in |
UL 746B |
DuPont Performance Polymers Rynite® FR515 BK507 PET
(Unverified Data**) Rynite® FR515 BK507 is a flame retardant 15% glass reinforced modified polyethtylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm(0.03in). Has a 140C temp index. Excellent balance of electr.. |
|||
UL RTI, Electrical | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL746B |
Covestro Apec® DP9-9331 High-Heat Polycarbonate, General Purpose
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
UL RTI, Electrical | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL746B |
Covestro Apec® DP9-9354 High-Heat Polycarbonate, Flame-Retardant
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
UL RTI, Electrical | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics ULTEM LTX300B PEI (Asia Pacific) Standard flow Polyetherimide blend with low toxicity, smoke, and flame evolution. ECO Compliant, UL94 V0 listing. |
|||
UL RTI, Electrical | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® 420 PBT (Asia Pacific) 30% GR, excellent strength, stiffness and dimensional stability. High heat resistance. Appliance handles, spotlights, electric motors, connectors. |
|||
UL RTI, Electrical | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® 735 PBT+PET 40% glass/mineral, excellent thermal performance/low shrink. Motorized heating appliances, adaptor rings, oven grills, etc. Black/natural only. |
|||
UL RTI, Electrical | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® EF4530 PBT (Asia Pacific) Easy flow, 30% glass-reinforced, PBTP resin. Flame retardant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
UL RTI, Electrical | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® IQ420 PBT (Asia Pacific) Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
UL RTI, Electrical | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Xenoy® 6370 PBT+PC (Europe-Africa-Middle East) XENOY 6370 is an impact modified semi-crystalline thermoplastic. blend with 30% glass fibre reinforcement offering toughness and ductility. |
|||
UL RTI, Electrical | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics LNP Thermocomp RF0057E PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RF0057E is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Non-Brominated & Non-Chlorinated Flame Retardant.Thi.. |
|||
UL RTI, Electrical | 140 °C | 284 °F | UL746B |
PlastxWorld CEVIAN® B5524 20% GF PBT/ABS Alloy Glass fiber reinforced and flame retarded PBT/ABS alloy.Information provided by PlastxWorld Inc. |
|||
UL RTI, Electrical | 140 °C | 284 °F | UL746B |
PlastxWorld CEVIAN® B5526 30% GF PBT/ABS Alloy Glass fiber reinforced and flame retarded PBT/ABS alloy.Information provided by PlastxWorld Inc. |
|||
UL RTI, Electrical | 140 °C | 284 °F | UL746B |
PlastxWorld CEVIAN® B5723 15% GF PBT/ABS Alloy Glass fiber reinforced, heat resistant and flame retarded PBT/ABS alloy.Information provided by PlastxWorld Inc. |
|||
UL RTI, Electrical | 140 °C | 284 °F | UL746B |
PlastxWorld CEVIAN® B5726 30% GF PBT/ABS Alloy Glass fiber reinforced, heat resistant and flame retarded PBT/ABS alloy.Information provided by PlastxWorld Inc. |
|||
UL RTI, Electrical | 140 °C | 284 °F | UL 746B |
Covestro Apec® 1697 High-Heat Polycarbonate This linear, amorphous copolycarbonate is most suitable for applications that must withstand high temperatures and exhibit toughness, impact resistance and high transparency. These properties, along.. |
|||
UL RTI, Electrical | 140 °C | 284 °F | UL 746B |
Covestro Apec® 1797 High-Heat Polycarbonate This linear, amorphous copolycarbonate is most suitable for applications that must withstand high temperatures and exhibit toughness, impact resistance and high transparency. These properties, along.. |
|||
UL RTI, Electrical | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL746B |
DSM Stanyl® 46HF5040 (DAM) Nylon 46 40% Glass Reinforced, Heat Stabilized, Flame Retardant, High Flow (North America) Information provided by DSM Engineering Plastics. |
|||
UL RTI, Electrical | 140 °C @Thickness 0.750 mm |
284 °F @Thickness 0.0295 in |
UL746B |
DSM Stanyl® TC153 PA46 FR(17) Thermal conductive material, Flame Retardant, Heat Stabilized |
|||
UL RTI, Electrical | 140 °C @Thickness 0.750 mm |
284 °F @Thickness 0.0295 in |
UL746B |
DSM Stanyl® TC154 PA46 FR(17) Thermal conductive material, Flame Retardant, Heat Stabilized |
|||
UL RTI, Electrical | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL746B |
DSM Stanyl® TE250F9 (DAM) Nylon 46 45% Glass Reinforced, Heat Stabilized, Flame Retardant (North America) Information provided by DSM Engineering Plastics. |
|||
UL RTI, Electrical | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
746B |
BASF Ultramid® 8234G HS BK 102 44% Glass Filled PA6 (Dry) Description Ultramid 8234G HS BK-102 is heat stabilized, pigmented black, 44% glass reinforced PA6 injection molding compound offering the highest level of strength, stiffness, high temperature perf.. |
|||
UL RTI, Electrical | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL 746B |
BASF Ultramid® B3UG4 Grey 22975 20% Glass Filled PA66 FR (Conditioned) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
UL RTI, Electrical | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL 746B |
BASF Ultramid® B3UG4 Grey 22975 20% Glass Filled PA66 FR (Dry) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
UL RTI, Electrical | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL 746B |
BASF Ultramid® B3UG4 LS BK 23215 20% Glass Filled PA66 FR (Dry) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
UL RTI, Electrical | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL 746B |
BASF Ultramid® B3UG4 LS Grey 22985 20% Glass Filled PA66 FR (Conditioned) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
UL RTI, Electrical | 140 °C @Thickness 6.00 mm |
284 °F @Thickness 0.236 in |
UL 746B |
DuPont Performance Polymers Rynite® 530 BK503 PET
(Unverified Data**) Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, .. |
|||
UL RTI, Electrical | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers Rynite® 530 BK503 PET
(Unverified Data**) Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, .. |
|||
UL RTI, Electrical | 140 °C @Thickness 2.00 mm |
284 °F @Thickness 0.0787 in |
UL 746B |
DuPont Performance Polymers Rynite® 530 BK503 PET
(Unverified Data**) Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, .. |