Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 6.47 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 6.47 GPa
938 ksi
ASTM D790
LATI LAPEX A G/20 20% Glass Fiber Reinforced Polyethersulfone (PES) (UL94 V-0)  (Unverified Data**)
Description: Lapex A compounds are polyethersulfone (PES) products. They are high temperature compounds offering an interesting combination of properties. Lapex A provides outstanding thermal resist..
Flexural Modulus 6.47 GPa
938 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP EFL24P PEI
LNP* LUBRICOMP* EFL24P is a compound based on Polyetherimide resin containing 20% Glass Fiber, 10% PTFE. Added features of this grade include: Wear Resistant, Exceptional Processing.
Flexural Modulus 6.47 GPa
939 ksi
ASTM D790
Samyang Tramid® 210G25 Polyamide, Reinforced
Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.210G25 is a reinforced grade.Applications:Automotive gear level housingConnectors..
Flexural Modulus 6.47 GPa
939 ksi
ASTM D790
Samyang Tramid® 215 Polyamide, High Impact
Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.215 is a high impact grade.Applications:Automotive knob types, door handles and m..
Flexural Modulus 6.47 GPa
938 ksi
ASTM D790
SABIC Innovative Plastics ULTEM JD4901 PEI (Asia Pacific)
Flexural Modulus 6.47 GPa
939 ksi
ASTM D790
PlastxWorld CEVIAN® B5524 20% GF PBT/ABS Alloy
Glass fiber reinforced and flame retarded PBT/ABS alloy.Information provided by PlastxWorld Inc.
Flexural Modulus 6.47 GPa
939 ksi
2.8mm/min; ASTM D790
Asia International Enterprise (Hong Kong) 60G4 Nylon 66, 20% Filled
Information provided by Asia International Enterprise (Hong Kong) Ltd.