Polymer Property : UL RTI, Mechanical without Impact = 266 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
UL RTI, Mechanical without Impact 130 °C
266 °F
UL 746C
Premix Premi-Glas® 1200H-30 Fiberglass Reinforced Thermoset SMC
Premi-Glas® 1200H-30 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:Go..
UL RTI, Mechanical without Impact 130 °C
266 °F
UL 746C
Premix Premi-Glas® 2205-15 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2205-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
UL RTI, Mechanical without Impact 130 °C
266 °F
UL 746C
Premix Premi-Glas® 2205-20 CRSX Polyester SMC
Premi-Glas® 2205-20 CR-SX is a 20% fiberglass reinforced Sheet Molding Compound formulated for condensate pan applications requiring chemical resistance, heat resistance, dimensional stability, we..
UL RTI, Mechanical without Impact 130 °C
266 °F
UL 746C
Premix Premi-Glas® 3101-10 Fiberglass Reinforced Thermoset BMC
Premi-Glas® 3101-10 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.Key features and ..
UL RTI, Mechanical without Impact 130 °C
266 °F
UL 746C
Premix Premi-Glas® 3200-25 Fiberglass Reinforced SMC
Description: Premi-Glas® 3200-25 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di..
UL RTI, Mechanical without Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 123R PC (Europe-Africa-Middle East)
LEXAN 123R is a low viscosity multi purpose U.V. stabilized grade and contains a release agent to ensure easy processing. LEXAN 123R is available in transparent, translucent and opaque colours.
UL RTI, Mechanical without Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 124 PC (Asia Pacific)
17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information and should not ..
UL RTI, Mechanical without Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 141R PC
UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 10.5 MFR. Internal mold release.
UL RTI, Mechanical without Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 241R PC (Asia Pacific)
10.5 MFR. Improved flame retardance. Internal mold release.
UL RTI, Mechanical without Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 500 PC
10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance.
UL RTI, Mechanical without Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 505R PC (Asia Pacific)
Lexan* 505R Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. Lexan 505R contains non-chlorinated, non-brominated flame retardant systems with UL-94 V0 rating at 1.5mm...
UL RTI, Mechanical without Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 923A PC (Asia Pacific)
Low viscosity, flame retardant with exceptional surface. Clear, tints and opaque colors. UV-stabilized.
UL RTI, Mechanical without Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 943A PC
Medium viscosity, superior flame retardance. UV-Stabilized. Clear, tints and opaque colors.
UL RTI, Mechanical without Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 943ASR PC
More robust design of standard 900 series flame retardant grade. Internal mold release. UV-stabilized.
UL RTI, Mechanical without Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 945ASR PC (Asia Pacific)
Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t..
UL RTI, Mechanical without Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 955AU PC
Lexan* 955AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a V0 UL rating and is UV stabilized, providing additiona..
UL RTI, Mechanical without Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer
Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin..
UL RTI, Mechanical without Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® HF1140R PC
High flow grade. Heat stabilized. Enhanced level of mold release. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported with biocompatib..
UL RTI, Mechanical without Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® HPS2S PC
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma steriliza..
UL RTI, Mechanical without Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® HPX4 PC Copolymer (Europe-Africa-Middle East)
Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP..
UL RTI, Mechanical without Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® LUX9130C PC COPOLYMER (Europe-Africa-Middle East)
Lexan* LUX9130C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and..
UL RTI, Mechanical without Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® LUX9136C PC COPOLYMER (Asia Pacific)
Lexan* LUX9136C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and..
UL RTI, Mechanical without Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics LNP KONDUIT OX10324 PPS (Asia Pacific)
Thermally conductive mineral filled PPS FR compound, with through-plane and in-plane thermal conductivity of 3.5 W/(m*K) and 15 W/(m*K) respectively, conforming to ASTM E 1461 test standard.
UL RTI, Mechanical without Impact 130 °C
266 °F
UL 746C
Premix Premi-Glas® 2103-10 CRSX Polyester BMC
Premi-Glas® 2103-10 CR-SX is a 10% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U..
UL RTI, Mechanical without Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 144R PC
UL rated HB. 200 series recommended when V-2 rating required. MFR 10.5. Internal mold release. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer ..
UL RTI, Mechanical without Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® LUX9132C PC COPOLYMER
Lexan* LUX9132C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and..
UL RTI, Mechanical without Impact 130 °C
266 °F
Samsung Cheil Industries Infino® EN-1052 PC, FR
Non-halogen flame-retardant material with high heat resistance that can be used in battery chargerInformation provided by Samsung Cheil Industries.
UL RTI, Mechanical without Impact 130 °C

@Thickness 1.47 mm
266 °F

@Thickness 0.0579 in
UL 746B
Teijin Panlite® G-3420R Glass Fiber Reinforced Polycarbonate Resin
GF 20% reinforced and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecision machinery components th..
UL RTI, Mechanical without Impact 130 °C

@Thickness 1.47 mm
266 °F

@Thickness 0.0579 in
UL 746B
Teijin Panlite® G-3430R Glass Fiber Reinforced Polycarbonate Resin
GF 30% reinforced and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecision machinery components th..
UL RTI, Mechanical without Impact 130 °C
266 °F
UL 746B
SABIC Innovative Plastics Lexan® 940A PC (Asia Pacific)
Medium viscosity, flame retardant PC. Exceptional surface. Clear, tints and opaque colors.