Material Notes:
CHO-SHIELD® 2054 silver-plated-copper filled commercial-grade coating proved high levels of EMI shielding effectiveness, abrasion resistance and excellent adhesion on a variety of materials used for electronic enclosures.Application: With their excellent leveling and uniformity, these coatings are compatible with all commercially available application technologies, including high volume/low pressure (HVLP) spray systems, and conventional propeller-agitated pressure pots. As low-settling compounds, they are ready for use after simple mixing in a paint shaker. They are supplied ready-to-spray, and don’t required additional thinning, although MEK can be used.Information provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 0.900 - 1.30 g/cc
0.900 - 1.30 g/cc
Volatile Organic Compounds (VOC) Content 750 g/l
750 g/l
Thickness >= 25.0 microns
>= 0.984 mil
Recommended
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Electrical Properties Metric English Comments
Surface Resistivity per Square <= 0.030 ohm

@Thickness 0.0250 mm
<= 0.030 ohm

@Thickness 0.000984 in
Shielding Effectiveness 55 dB

@Frequency 2.00e+7 Hz
55 dB

@Frequency 2.00e+7 Hz
26 in. x 26 in. test panel; TP08 Modified
77 dB

@Frequency 1.00e+8 Hz
77 dB

@Frequency 1.00e+8 Hz
26 in. x 26 in. test panel; TP08 Modified
83 dB

@Frequency 1.00e+9 Hz
83 dB

@Frequency 1.00e+9 Hz
26 in. x 26 in. test panel; TP08 Modified
88 dB

@Frequency 1.00e+10 Hz
88 dB

@Frequency 1.00e+10 Hz
26 in. x 26 in. test panel; TP08 Modified
90 dB

@Frequency 2.00e+8 Hz
90 dB

@Frequency 2.00e+8 Hz
26 in. x 26 in. test panel; TP08 Modified
92 dB

@Frequency 4.00e+9 Hz
92 dB

@Frequency 4.00e+9 Hz
26 in. x 26 in. test panel; TP08 Modified
Processing Properties Metric English Comments
Cure Time 5.00 min

@Temperature 24.0 °C
0.0833 hour

@Temperature 75.2 °F
Followed by 30 min @ 60°-71°C
1440 min

@Temperature 24.0 °C
24.0 hour

@Temperature 75.2 °F
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Consistency Thin Fluid
Filler Silver-Plated Copper and Pure Silver Flakes
Mix 1-part
Polymer Acrylic
Theoretical Coverage 192 ft2/gal
Viscosity #2 Zahn Cup 14-19 sec
Suggested