Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.900 g/cc | 0.900 g/cc | |
Radici Heraflex® A 90-11-44 UV TPS-SEBS Thermoplastic Elastomer TPS-SEBS Thermoplastic Elastomer. 92 Shore A, low odor level and stable to light. Scratch resistance, dry grip.Application examples: Cover for hand brake leverProcessing technology: Injection moldin.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ISO 1183 |
Solvay Engineered Polymers DEXFLEX® 810HS TPO
(discontinued **) Description: DEXFLEX® 810HS is a thermoplastic olefinic elastomer (TPO) that offers excellent weatherability, paintability and processability. This material is designed to exceed the requirements .. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | |
Radici Heraflex® A 40-11-91 TPS-SEBS Thermoplastic Elastomer TPS-SEBS Thermoplastic Elastomer. 40 Shore A. Low density, rubber like surface, easy flowing.Application examples: Soft gripsProcessing technology: Injection moldingInformation provided by Radici gr.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 1404-01 Polypropylene High Impact Polypropylene DescriptionPolypropylene PP 1404-01 is a medium flow, high-impact polypropylene for injection molded parts. Information provided by A. Schulman. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 3487-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3487-01 is a special homopolymer polypropylene formulated with a long term heat aging resistance. This material has excellent resistance to chemicals and solvents. High.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 1404-01 Polypropylene High Impact Polypropylene DescriptionPolypropylene PP 1404-01 is a medium flow, high-impact polypropylene for injection molded parts. Information provided by A. Schulman. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 1579 Polypropylene Impact Grade Polypropylene DescriptionPolypropylene PP 1579 is an impact grade of polypropylene for use in parts which require good impact and good appearance in light weight injection molded parts. Information provided by A.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 3466-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3466-01 is a homopolymer polypropylene with the addition of antistatic. This product enhances processing with fast cycle times in injection molding.ApplicationPP 3466-01.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 828-01 Polypropylene Molding Grade Impact Polypropylene DescriptionPolypropylene PP 828-01 is a molding grade impact polypropylene. ApplicationThis material meets the FDA Regulation 21 CFR 177.1520 for food contact applications. Information provided by .. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 828-31 Polypropylene Black Molding Grade Impact Polypropylene DescriptionPolypropylene PP 828-31 Black is a molding grade impact polypropylene.Information provided by A. Schulman. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 829-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 829-01 is a homopolymer polypropylene approved to Ford specification ESB-M4D63A. Primarily used for interior automotive components, this material is also well suited for.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PX 1040 Information provided by A. Schulman. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 1248-01 Polypropylene High-Flow Homopolymer Polypropylene DescriptionPolypropylene PP 1248-01 is a high-flow homopolymer polypropylene nucleated and anti static designed for the high speed molding of thin-walled, multi-cavity parts. ApplicationTypical appl.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 1579 Polypropylene Impact Grade Polypropylene DescriptionPolypropylene PP 1579 is an impact grade of polypropylene for use in parts which require good impact and good appearance in light weight injection molded parts. Information provided by A.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 3475-01 Polypropylene High Melt Homopolymer Polypropylene DescriptionPolypropylene PP 3475-01 Natural is a high melt homopolymer polypropylene with consistent general purpose homopolymer characteristics. Information provided by A. Schulman. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 3486-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3486-01 is a special homopolymer polypropylene designed with long term heat aging formula for appliance application.ApplicationThis product is for injection molded applic.. |
|||
Specific Gravity | 0.900 - 0.920 g/cc | 0.900 - 0.920 g/cc | |
Westlake Epolene® C-13P Coating Grade - Branched Medium Molecular Weight Polyethylene Polymer Description: Epolene C-13P is a branched low density polyethylene homopolymer powder with low color and medium molecular weight. It is useful as a base polymer for adhesives and coatings, color con.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 3726 Information provided by A. Schulman. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 1407H-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1407H-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 1407H-01 meets FDA Regulation 21 CFR 177.1520 for food contact .. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 3052UX Impact Resistant Copolymer DescriptionPolyfort® PP 3052UX is a UV stabilized extra high flow impact resistant copolymer with a relatively high stiffness.Information provided by A. Schulman. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 1407H-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1407H-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 1407H-01 meets FDA Regulation 21 CFR 177.1520 for food contact .. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 1621 Polypropylene Low Flow Homopolymer Polypropylene DescriptionPolypropylene PP 1621 is a low flow homopolymer polypropylene primarily used for sheet strapping and profile extrusion applications.ApplicationPP 1621 meets FDA Regulation 21 CFR 177.1520.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
Teknor Apex Uniprene® UN-2420H Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Blue Tint P40530 Concentrate Based In Homopolymer Polypropylene DescriptionPOLYBATCH® P40530 is a blue tint color concentrate based in homopolymer polypropylene. This concentrate was designed to provide color in blow molding applications. POLYBATCH® P40530 i.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 3449-01 Polypropylene Copolymer Polypropylene DescriptionPolypropylene PP 3449-01 is a new generation copolymer polypropylene utilizing unique catalyst technology. Combining an excellent balance of high stiffness and impact. This product inc.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D 792 |
CPT C-Flex® R70-003 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D 792 |
CPT C-Flex® R70-051 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D 792 |
CPT C-Flex® R70-081 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | 15°C |
ExxonMobil SAE 30 Mobilgard ADL Series Mobilgard ADL Series by ExxonMobil is a high performance family of increased dispersancy engine oils for high BMEP medium and high-speed diesel engines operating on distillate and MDO fuels. These a.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
Aaron Industries AAROLENE® ARPP H 200-1 PP Black Polypropylene Homopolymer Compounded Resin AAROLENE® ARPP 200 Series Polypropylene Compounded ResinFeatures: A pre-colored, black homopolymer polypropylene resin specifically designed for all injection molding applications.High Flow |