Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.900 g/cc | 0.900 g/cc | 23/23°C; ASTM D792 |
RheTech Products FT1001-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Facias, claddings, and rocker panelsBodyside moldingsStep pads and bumper componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | 23/23°C; ASTM D792 |
RheTech Products FT2700-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Air deflectorsFuel filler shieldsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | 23/23°C; ASTM D792 |
RheTech Products P102-00 Polypropylene, Black Applications: Consumer goodsIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D1505 |
LG Chemical SEETEC M1500 Polypropylene Impact Copolymer SEETEC M1500 is a heterophasic polypropylene copolymer for injection molding applications. SEETEC M1500 exhibits a high flowability and a good balance of stiffness and impact strength. SEETEC M1500 .. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D4025 |
Kraton® G1657 M (SEBS) Linear Triblock Copolymer Description: Kraton G1657 M is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 13% . It is supplied from North America in the physical form id.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
Kraton® G1730 M (SEP) Linear Diblock Copolymer Description: Kraton G1730 M is a clear copolymer based on styrene and ethylene/propylene with a polystyrene content of 21%. It is supplied from North America in the physical form identified: Kraton .. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ISO 1183 |
MRC Polymers MAXTEL™ 620-BK Polypropylene Copolymer • For injection molding• Excellent process ability with high flow and high impact.Information provided by MRC Polymers Inc. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
STAR Thermoplastic Alloys & Rubbers StarMediflex P 7020-1000 TPE Product Description: StarMediflex P 7020-1000 is an easy processing TPE designed for injection molding. This particular class of TPE material for medical products and tubing applications. Features:S.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 1901-01 Polypropylene High-Flow Homopolymer Polypropylene DescriptionPolypropylene PP 1901-01 is a high-flow homopolymer polypropylene designed for the high-speed molding of thin walled, multi-cavity parts. ApplicationTypical applications of PP 1901-01 ar.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 3353-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 3353-01 is a high flow medium impact polypropylene which is suitable for molding thin parts with long mold flow distances. It permits reduction of cycle times, temperatu.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 3457-01 Copolymer Polypropylene DescriptionPolypropylene PP 3457-01 is a copolymer polypropylene combining high impact at cold temperatures while maintaining stiffness. Ideal for durables in such applications for the furniture, a.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 3488-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3488-01 is a specially formulated homopolymer polypropylene designed for large appliance injection molding. This material has excellent chemical resistance in addition t.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 1102-01 Polypropylene General Purpose, Molding Grade Polypropylene DescriptionPolypropylene PP 1102-01 is a general purpose, molding grade with UL 94 HB approval for use in large and thin wall applications. ApplicationPolypropylene PP 1102-01 meets FDA Regulation.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 3457-01 Copolymer Polypropylene DescriptionPolypropylene PP 3457-01 is a copolymer polypropylene combining high impact at cold temperatures while maintaining stiffness. Ideal for durables in such applications for the furniture, a.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 3471-01 Polypropylene High Flow Homopolymer Polypropylene DescriptionPolypropylene PP 3471-01 is an ultra high flow homopolymer polypropylene designed for high speed, thin wall injection molding.Information provided by A. Schulman. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 3468-01 Polypropylene Homopolymer For High Speed Extrusion DescriptionPolypropylene PP 3468-01 is a specially designed homopolymer for high speed extrusion applications. ApplicationTypical applications of PP 3468-01 include profile extrusions, strapping, r.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 3490-01G Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3490-01G Natural is a homopolymer for extrusion and compounding applications. This material can also be used as a carrier resin for color concentrates. ApplicationPP 349.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 1404-01 Polypropylene High Impact Polypropylene DescriptionPolypropylene PP 1404-01 is a medium flow, high-impact polypropylene for injection molded parts. Information provided by A. Schulman. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 3466-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3466-01 is a homopolymer polypropylene with the addition of antistatic. This product enhances processing with fast cycle times in injection molding.ApplicationPP 3466-01.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 1500X-01 Polypropylene High Impact Copolymer Polypropylene DescriptionPolypropylene PP 1500X-01 is a specially formulated high impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 3486-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3486-01 is a special homopolymer polypropylene designed with long term heat aging formula for appliance application.ApplicationThis product is for injection molded applic.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 3466-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3466-01 is a homopolymer polypropylene with the addition of antistatic. This product enhances processing with fast cycle times in injection molding.ApplicationPP 3466-01.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 1579 Impact Grade Polypropylene DescriptionPolyfort® PP 1579H is an impact grade of polypropylene for use in parts which require good impact and good appearance in light-weight injection molded parts. Information provided by A. .. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 984 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 984 is a medium impact polypropylene used primarily for automotive parts subjected to impact.Information provided by A. Schulman. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D 792 |
CPT C-Flex® R70-072 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ExxonMobil Method |
ExxonMobil Exxelor™ VA 1202 Low Viscosity Ethylene Copolymer Product Description: Exxelor VA 1202 polymer resin is a low viscosity ethylene copolymer functionalized with maleic anhydride by reactive extrusion. Its fully saturated backbone results in outstan.. |
|||
Specific Gravity | 0.900 g/cc @Temperature 23.0 °C |
0.900 g/cc @Temperature 73.4 °F |
ASTM D792 |
Amco PRIMATOP PP CO 350-40 Polypropylene Copolymer PP CO 350-40 features impact resistance and low temperature stiffness. Applications include injection molding and containers.Former A-Top Polymers product; part of Amco product line since 2013. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 3052UX Impact Resistant Copolymer DescriptionPolyfort® PP 3052UX is a UV stabilized extra high flow impact resistant copolymer with a relatively high stiffness.Information provided by A. Schulman. |
|||
Specific Gravity | 0.900 g/cc | 0.900 g/cc | ASTM D792 |
A. Schulman PP 1407H-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1407H-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 1407H-01 meets FDA Regulation 21 CFR 177.1520 for food contact .. |