Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 55 dB @Frequency 10000 Hz |
55 dB @Frequency 10000 Hz |
H-Field |
P & P Technology Oriented Wires In Silicone P & P Technology SP, SS, SR, SW & SF Ranges of gasket materials consist of Monel or aluminum wires embedded into solid silicone, sponge silicone or fluorosilicone, a fire retardant variant is also a.. |
|||
Shielding Effectiveness | 55 dB @Frequency 4.00e+7 Hz |
55 dB @Frequency 4.00e+7 Hz |
With 360° ground termination |
Parker Chomerics CHO-JAC CJ-021 Flat Cable EMI Shield Flat Cable EMI Shield. Cho-Jack® shielding is a high quality flat cable jacket designed to attenuate RF signals and bring digital electronic devices into compliance with FCC and TEMPEST radiated em.. |
|||
Shielding Effectiveness | 55 dB @Frequency 1.00e+8 Hz |
55 dB @Frequency 1.00e+8 Hz |
With 360° ground termination |
Parker Chomerics CHO-JAC CJ-021 Flat Cable EMI Shield Flat Cable EMI Shield. Cho-Jack® shielding is a high quality flat cable jacket designed to attenuate RF signals and bring digital electronic devices into compliance with FCC and TEMPEST radiated em.. |
|||
Shielding Effectiveness | 55 dB @Frequency 4.00e+8 Hz |
55 dB @Frequency 4.00e+8 Hz |
With 360° ground termination |
Parker Chomerics CHO-JAC CJ-022 Flat Cable EMI Shield Flat Cable EMI Shield. Cho-Jack® shielding is a high quality flat cable jacket designed to attenuate RF signals and bring digital electronic devices into compliance with FCC and TEMPEST radiated em.. |
|||
Shielding Effectiveness | 55 dB @Frequency 4.00e+8 Hz |
55 dB @Frequency 4.00e+8 Hz |
360° Ground Termination |
Parker Chomerics CHO-JAC® CJ-022 Flat Cable EMI Shield Description: CHO-JAC shielding is a high quality flat cable jacket designed to attenuate RF signals and bring digital electronic devices into EMC compliance at an attractive cost. It is lightweight .. |
|||
Shielding Effectiveness | >= 55 dB @Frequency 200000 Hz |
>= 55 dB @Frequency 200000 Hz |
H Field; MIL-DTL-83528 Para.4.6.12 |
Parker Chomerics CHO-SEAL 1287 Conductive Elastomer Conductive Fluorosilicone EMI/EMP Gasket. This material is silver-plated-aluminum-filled fluorosilicone elastomer which provides pressure and environmental sealing as well as high levels of EMI shie.. |
|||
Shielding Effectiveness | >= 55 dB @Frequency 200000 Hz |
>= 55 dB @Frequency 200000 Hz |
H Field; MIL-DTL-83528 Para.4.6.12 |
Parker Chomerics CHO-SEAL 1298 EMI Shielding Material Corrosion Resistant EMI Shielding Gasket. Through the use of new proprietary particle painting and elastomer compounding technology, CHO-SEAL® 1298 shielding elastomer offers a six-fold increase in.. |
|||
Shielding Effectiveness | 55 dB @Frequency 2.00e+7 Hz |
55 dB @Frequency 2.00e+7 Hz |
26 in. x 26 in. test panel; TP08 Modified |
Parker Chomerics CHO-SHIELD® 2056 Conductive Coating CHO-SHIELD® 2054 silver-plated-copper filled commercial-grade coating proved high levels of EMI shielding effectiveness, abrasion resistance and excellent adhesion on a variety of materials used fo.. |
|||
Shielding Effectiveness | 55 dB @Frequency 1.00e+9 Hz |
55 dB @Frequency 1.00e+9 Hz |
14" x 14" open aperture; MIL-STD-285; CHO-TM-TPO8 |
Parker Chomerics WIN-SHIELD™ Elite EMI Shielded Window Description: Shielded Windows WIN-SHIELD™ EMI shielded windows provide exceptional optical performance without sacrificing EMI shielding. This new generation of shielded windows is designed specif.. |
|||
Shielding Effectiveness | 55 dB @Frequency 3.00e+8 Hz |
55 dB @Frequency 3.00e+8 Hz |
|
Parker Chomerics WIN-SHIELD™ Mesh 100 EMI Shielding Mesh Blackened copper plating. WIN-SHIELD Mesh 100 provides exceptional shielding performance and can be used as an optical product, to cover airflow openings, to wrap cable or other applications where .. |
|||
Shielding Effectiveness | 55 dB @Frequency 100000 Hz |
55 dB @Frequency 100000 Hz |
H-Field |
Parker Chomerics Tecknit Consil®-A 897 Silver-Aluminum Filled Silicone Elastomer Description: CONSIL-A is a silicone or fluorosilicone elastomer filled with silver-plated aluminum particles designed to achieve maximum electrical conductivity. CONSIL-A provides high shielding eff.. |
|||
Shielding Effectiveness | 55 dB @Frequency 100000 Hz |
55 dB @Frequency 100000 Hz |
H-Field |
Parker Chomerics Tecknit Teckshield®-F 100 OPI 0.002" Diameter Wire, Allycarbonate EMI Shielding Window Description: Tecknit Allylcarbonate shielded windows are manufactured by casting a woven EMI shield mesh into a material that has optical properties similar to that of glass. The window offers a lig.. |
|||
Shielding Effectiveness | 55 dB @Frequency 100000 Hz |
55 dB @Frequency 100000 Hz |
H-Field |
Parker Chomerics Tecknit Teckshield®-F 100 OPI 0.0022" Diameter Wire, High Performance EMC Window Description: TECKSHIELD-F high-performance fully laminated flat windows are specially designed to provide optimum optical transmission and EMI shielding in severe interference environments. TECKSHIE.. |
|||
Shielding Effectiveness | 55 dB @Frequency 100000 Hz |
55 dB @Frequency 100000 Hz |
H-Field |
Parker Chomerics Tecknit Teckshield®-F 145 OPI 0.0022" Diameter Wire, High Performance EMC Window Description: TECKSHIELD-F high-performance fully laminated flat windows are specially designed to provide optimum optical transmission and EMI shielding in severe interference environments. TECKSHIE.. |
|||
Shielding Effectiveness | 55 dB @Thickness 3.00 mm |
55 dB @Thickness 0.118 in |
SABIC Method |
SABIC Innovative Plastics LNP Faradex EX06464 PEI (Asia Pacific) LNP* Faradex* EX06464 is a compound based on Polyetherimide resin containing Stainless Steel. Added features of this material include: Electrically
Conductive, EMI/RFI Shielding.This data was suppli.. |
|||
Shielding Effectiveness | 55 - 65 dB @Thickness 3.00 mm |
55 - 65 dB @Thickness 0.118 in |
SABIC Method |
SABIC Innovative Plastics LNP Faradex EX06464 PEI (Asia Pacific) LNP* Faradex* EX06464 is a compound based on Polyetherimide resin containing Stainless Steel. Added features of this material include: Electrically
Conductive, EMI/RFI Shielding.This data was suppli.. |
|||
Shielding Effectiveness | 55 dB @Frequency 5.00e+9 Hz |
55 dB @Frequency 5.00e+9 Hz |
1/8 thickness |
PolyOne Stat-Tech™ ST9620-0020 ES Red Liquid Crystal Polymer + PPS (LCP+PPS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Shielding Effectiveness | 55 dB @Frequency 2.00e+9 Hz |
55 dB @Frequency 2.00e+9 Hz |
CHO-TP08 |
Parker Chomerics CHO-FORM 5531 EMI Shielding Material One component, moisture cure, form-in-place EMI gasketing material. This electrically conductive formulation contains silver-plated copper particles dispersed in a silicone elastomer. It is designed.. |