Polymer Property : Specific Gravity = 1.30 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.24 - 1.30 g/cc
1.24 - 1.30 g/cc
ASTM D792
S&E Specialty Polymers GA-1941-AFRO PVC
Application: 105° C PVC insulating compound designed for SJEOO applicationsInformation provided by S&E Specialty Polymers
Specific Gravity 1.24 - 1.30 g/cc
1.24 - 1.30 g/cc
ASTM D792
S&E Specialty Polymers GA-509ORLT PVC
Application: Lead free, flame retardant UV and oil resistant PVC jacketing compound with superior low temperature properties.Information provided by S&E Specialty Polymers
Specific Gravity 1.24 - 1.30 g/cc
1.24 - 1.30 g/cc
ASTM D792
S&E Specialty Polymers TufFlex™ GF 3161 PNU TPE Compound
Application: High performance oil, gasoline & chemical resistant boot upper compound.Information provided by S&E Specialty Polymers
Specific Gravity 1.24 - 1.30 g/cc
1.24 - 1.30 g/cc
ASTM D792
S&E Specialty Polymers TufFlex™ GTPE-2272 TPE Compound
Application: A 105°C flexible, oil resistant, flame retardant TPE jacketing material designed for SJEO applications.Information provided by S&E Specialty Polymers
Specific Gravity 1.10 - 1.30 g/cc
1.10 - 1.30 g/cc
PolyChem Alloy PolyGard 3005R
PolyFoam decomposes when heated to create a uniform microcellular structure. It can be used in extrusion and injection molding processes to reduce weight in parts without adversely affecting the ph..
Specific Gravity 0.900 - 1.30 g/cc
0.900 - 1.30 g/cc
Parker Chomerics CHO-SHIELD® 2056 Conductive Coating
CHO-SHIELD® 2054 silver-plated-copper filled commercial-grade coating proved high levels of EMI shielding effectiveness, abrasion resistance and excellent adhesion on a variety of materials used fo..
Specific Gravity 1.20 - 1.30 g/cc
1.20 - 1.30 g/cc
PolyChem Alloy AquaGard™ 3004M
AquaGard products are designed to improve the flame retardency of polyolefins without the use of halogen additives, such as bromine or chlorine. AquaGard products are available in a polyethylene ..
Specific Gravity 1.20 - 1.30 g/cc

@Thickness 1.57 mm
1.20 - 1.30 g/cc

@Thickness 0.0620 in
ASTM D792
Industrial Laminates/Norplex NP101 Synthetic Fabric
Description: Phenolic resin combined with spun nylon fabric. Good impact strength and excellent electrical properties under high humidity conditions. Meets applicable Boeing specification, but exemp..
Specific Gravity 1.24 - 1.30 g/cc
1.24 - 1.30 g/cc
ASTM D 792
Karina 701D25-1-A-IS Natural PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.24 - 1.30 g/cc
1.24 - 1.30 g/cc
ASTM D 792
Karina 722-48/1-A-IS Black PVC Compound
Heavy metal free PVC compound recommended for extrusion of automobile profilesInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.24 - 1.30 g/cc
1.24 - 1.30 g/cc
ASTM D 792
Karina 771-48/1-BY-IS Black PVC Compound
Weather resistant PVC compound, recommended for injection and extrusion of automotive profilesInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.26 - 1.30 g/cc
1.26 - 1.30 g/cc
ASTM D 792
Karina 800D48/1-A-IS-BZ Black PVC Compound
Heavy metal free PVC compound recommended for injection and extrusion of automotive parts.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.24 - 1.30 g/cc
1.24 - 1.30 g/cc
NBR NM-IEC 60811-1-3
Karina E 42/183-FC-LMP Red Color Concentrate for PVC
Color concentrate recommended for application in PVC compounds for electrical wires and cables. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes.Important con..
Specific Gravity 1.24 - 1.30 g/cc
1.24 - 1.30 g/cc
ASTM D 792
Karina E 57/200-D-AT-IS-SD Clear PVC Compound
PVC compound recommended for shrink films.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.24 - 1.30 g/cc
1.24 - 1.30 g/cc
ASTM D 792
Karina E 680D35/1-B-IS Ivory PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.24 - 1.30 g/cc
1.24 - 1.30 g/cc
ASTM D 792
Karina 57/200-D-AT-IS-SD Clear PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.24 - 1.30 g/cc
1.24 - 1.30 g/cc
ASTM D 792
Karina E 57/201-D-IS-SD Compound PVC Crystal
Clear/crystal PVC compound specially developed for skin films.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.27 - 1.30 g/cc
1.27 - 1.30 g/cc
ASTM D792
Spartech Royalite R47 PVC Alloy Fire Rated Sheet
Description: Fire Rated SheetInformation provided by Spartech.
Specific Gravity 1.27 - 1.30 g/cc
1.27 - 1.30 g/cc
ASTM D792
Spartech Royalite R522 PVC Alloy Aircraft Grade Sheet
Description: Aircraft Grade SheetInformation provided by Spartech.
Specific Gravity 1.26 - 1.30 g/cc
1.26 - 1.30 g/cc
ASTM D792
Compuestos Dominicanos Polycom C-051065 PVC Compound
Compuestos Dominicanos SA produces a wide variety of PVC compounds for the injection molding of footwear products; everything from full injection, shoe soles, boots, and PVC compounds for oil resist..
Specific Gravity 1.26 - 1.30 g/cc
1.26 - 1.30 g/cc
ASTM D-792
Axiall 8560 Moldings & Extrusions Flexible PVC
A clear, semi-rigid extrusion or molding grade compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.26 - 1.30 g/cc
1.26 - 1.30 g/cc
ASTM D-792
Axiall 11470 Wire & Cable Flexible PVC
Highly flame retardant clear compound. Recommended as jacket in PVC/PVC VW-1 constructions.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.26 - 1.30 g/cc
1.26 - 1.30 g/cc
ASTM D-792
Axiall 8780 Moldings & Extrusions Flexible PVC
Low gravity, general purpose extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.26 - 1.30 g/cc
1.26 - 1.30 g/cc
ASTM D-792
Axiall 19740 Wire & Cable Flexible PVC
Non-lead stabilized, 105°C rated insulation compound with excellent low temperature properties. Suitable for use in Class 43 applications. Also suitable for injection molding applications.Informa..
Specific Gravity 0.900 - 1.30 g/cc
0.900 - 1.30 g/cc
Parker Chomerics CHO-SHIELD® 2052 Conductive Coating
CHO-SHIELD® 2052 silver-plated-copper filled commercial-grade coating proved high levels of EMI shielding effectiveness, abrasion resistance and excellent adhesion on a variety of materials used fo..
Specific Gravity 1.26 - 1.30 g/cc
1.26 - 1.30 g/cc
ASTM D-792
Axiall 8681 Moldings & Extrusions Flexible PVC
General purpose, elastomeric vinyl compound well suited for co-extrusion with rigid PVC.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.26 - 1.30 g/cc
1.26 - 1.30 g/cc
NBR NM-IEC 60811-1-3
Karina 02/223-G Yellow Color Concentrate for PVC
Color concentrate recommended for application in PVC compounds for general purposes injection. Recommended to use 2%.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.26 - 1.30 g/cc
1.26 - 1.30 g/cc
ASTM D 792
Karina CAK 55-48/1 Black PVC Compound
Reclaimed PVC compound recommended for injection of footwear soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.26 - 1.30 g/cc
1.26 - 1.30 g/cc
ASTM D-792
Axiall 18650 Moldings & Extrusions Flexible PVC
General purpose compound recommended for 105C applications. Well suited for 105C molding and general purpose extrusions.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in..
Specific Gravity 1.24 - 1.30 g/cc
1.24 - 1.30 g/cc
ASTM D 792
Karina E 57/200-D-AT-IS-SI-SD Clear PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.