Parker Chomerics CHO-SEAL® 6308 Conductive Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone
Manufacturer Parker Chomerics
Trade Name CHO-SEAL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-SEAL® 6308 Conductive Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Extruded onlyRoHS CompliantInformation provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 1.75 - 2.25 g/cc
1.75 - 2.25 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 55 - 75
55 - 75
ASTM D2240
Tensile Strength >= 1.38 MPa
>= 200 psi
ASTM D412
Elongation at Break >= 75 %
>= 75 %
ASTM D412
Tear Strength <= 7.01 kN/m
<= 40.0 pli
ASTM D624
Compression Set <= 30 %

@Temperature 100 °C,
Time 252000 sec
<= 30 %

@Temperature 212 °F,
Time 70.0 hour
ASTM D395, Method B
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Flex TR10
Electrical Properties Metric English Comments
Volume Resistivity <= 0.10 ohm-cm
<= 0.10 ohm-cm
without pressure-sensitive adhesive; CEPS-0002
Shielding Effectiveness >= 100 dB

@Frequency 1.00e+8 Hz
>= 100 dB

@Frequency 1.00e+8 Hz
E-Field; Method 1, CHO-TM-TP08
>= 100 dB

@Frequency 5.00e+8 Hz
>= 100 dB

@Frequency 5.00e+8 Hz
E-Field; Method 1, CHO-TM-TP08
>= 100 dB

@Frequency 2.00e+9 Hz
>= 100 dB

@Frequency 2.00e+9 Hz
Plane Wave; Method 1, CHO-TM-TP08
>= 100 dB

@Frequency 1.00e+10 Hz
>= 100 dB

@Frequency 1.00e+10 Hz
Plane Wave; Method 1, CHO-TM-TP08
Descriptive Properties Value Comments
Binder Silicone
Filler Ni/C
Heat Aging <0.25 ohm-cm
150°C for 48 hr, CEPS-0002