Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 100 dB @Thickness 1.60 mm, Frequency 5.00e+8 Hz |
100 dB @Thickness 0.0630 in, Frequency 5.00e+8 Hz |
MIL G83528 |
Rogers Corporation Bisco® EC-2130 Conductive Silicone Base Polymer: SiliconeFiller: Nickel-GraphiteApplications: Silicone EMI ShieldsThickness: 0.063 inches and 0.125 inchesInformation provided by Rogers Corporation. |
|||
Shielding Effectiveness | 100 dB @Frequency 1.00e+8 Hz |
100 dB @Frequency 1.00e+8 Hz |
Mil-G-83528/Mil std 285 |
P & P Technology EC-H Silver Copper Loaded Silicone P & P Technology material reference EC-H is a printing grade silicone elastomer with a Silver/Copper conductive filler and is Tan in color. The material is specially compounded to offer excellent p.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 1.00e+7 Hz |
>= 100 dB @Frequency 1.00e+7 Hz |
E-Field |
P & P Technology Monex Expanded Monel Foil Monex is an expanded monel foil of uniform thickness (0.5mm or 0.75mm available) which is manufactured to give a large number of contact points per cm². It can be supplied with a filler of silicon.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 1.00e+8 Hz |
>= 100 dB @Frequency 1.00e+8 Hz |
E-Field |
P & P Technology Monex Expanded Monel Foil Monex is an expanded monel foil of uniform thickness (0.5mm or 0.75mm available) which is manufactured to give a large number of contact points per cm². It can be supplied with a filler of silicon.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 5.00e+8 Hz |
>= 100 dB @Frequency 5.00e+8 Hz |
MIL-DTL-83528 Para.4.6.12 |
Parker Chomerics CHO-SEAL 1401 Conductive Elastomer High performance for non-corrosive environments; soft(45 Shore A) for low closure force where gasket geometry cannot be exploited; low tear strength; no fluid resistance. Molded and ExtrudedRoHS Com.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 1.00e+8 Hz |
>= 100 dB @Frequency 1.00e+8 Hz |
E Field; CHO-TM-TP08 |
Parker Chomerics CHO-SEAL 6370 Conductive Elastomer Commercial Grade Conductive Elastomer Extrusions. These materials offer excellent cost/performance characteristics for commercial EMI gasket applications. These silicone and fluorosilicone based con.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 5.00e+8 Hz |
>= 100 dB @Frequency 5.00e+8 Hz |
CHO-TM-TP08 |
Parker Chomerics CHO-SEAL L6303 Conductive Elastomer Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Molded and ExtrudedRoHS CompliantInformation provid.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 1.00e+8 Hz |
>= 100 dB @Frequency 1.00e+8 Hz |
E-Field; Method 1, CHO-TM-TP08 |
Parker Chomerics CHO-SEAL® 6308 Conductive Elastomer Description: Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Extruded onlyRoHS CompliantInformation.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 5.00e+8 Hz |
>= 100 dB @Frequency 5.00e+8 Hz |
E-Field; Method 1, CHO-TM-TP08 |
Parker Chomerics CHO-SEAL® 6308 Conductive Elastomer Description: Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Extruded onlyRoHS CompliantInformation.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 1.00e+10 Hz |
>= 100 dB @Frequency 1.00e+10 Hz |
Plane Wave; Method 3, CHO-TM-TP09 |
Parker Chomerics CHO-SEAL® 6503 Conductive Elastomer Description: Highest performance in harsh environments; excellent shielding; best choice for corrosion requirements against aluminum.Molded and ExtrudedRoHS CompliantInformation provided by Chomeric.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 1.00e+10 Hz |
>= 100 dB @Frequency 1.00e+10 Hz |
Plane Wave; Method 3, CHO-TM-TP09 |
Parker Chomerics CHO-SEAL® 6510 Conductive Elastomer Extruded onlyInformation provided by Chomerics |
|||
Shielding Effectiveness | >= 100 dB @Frequency 1.00e+9 Hz |
>= 100 dB @Frequency 1.00e+9 Hz |
Plane Wave |
Parker Chomerics Tecknit Consil®-E 811 Extruded Silver-Filled Silicone Elastomer Description: CONSIL-E is a continuously extruded silicone elastomer filled with silver-plated inert particles. It is a medium hardness material providing high electrical conductivity and moisture se.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 1.00e+9 Hz |
>= 100 dB @Frequency 1.00e+9 Hz |
Plane Wave |
Parker Chomerics Tecknit Consil®-E 815 Extruded Silver-Filled Silicone Elastomer Description: CONSIL-E is a continuously extruded silicone elastomer filled with silver-plated inert particles. It is a medium hardness material providing high electrical conductivity and moisture se.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 1.00e+9 Hz |
>= 100 dB @Frequency 1.00e+9 Hz |
Plane Wave |
Parker Chomerics Tecknit Consil®-II 841 Molded Silver-Filled Silicone Elastomer Description: CONSIL-II is a molded silicone elastomer filled with silver-coated inert particles. It provides high electrical conductivity, broadband shielding and moisture sealing. CONSIL-II is desi.. |
|||
Shielding Effectiveness | 100 dB @Frequency 1.00e+10 Hz |
100 dB @Frequency 1.00e+10 Hz |
Plane Wave |
Parker Chomerics Tecknit Consil®-N 891 Silver-Nickel Filled Silicone Elastomer Description: CONSIL-N is a silicone elastomer filled with silver-plated nickel particles and designed to provide high shielding effectiveness and corrosion resistance. CONSIL-N is available in sheet.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 1.00e+9 Hz |
>= 100 dB @Frequency 1.00e+9 Hz |
Plane Wave |
Parker Chomerics Tecknit Consil®-R 856 Pure Silver-Filled Silicone Elastomer Description: CONSIL-R 856 offers the lowest durometer available for pure silver-filled elastomerTypical Applications: CONSIL-R is designed for use in low to moderate pressure applicationsInformation.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 1.00e+9 Hz |
>= 100 dB @Frequency 1.00e+9 Hz |
Plane Wave |
Parker Chomerics Tecknit Consil®-R 857 Pure Silver-Filled Silicone Elastomer Description: CONSIL-R 857 provides similar properties as 856, with a high durometerTypical Applications: CONSIL-R is designed for use in low to moderate pressure applicationsInformation provided by .. |
|||
Shielding Effectiveness | 100 dB @Frequency 100000 Hz |
100 dB @Frequency 100000 Hz |
H-Field |
Parker Chomerics Tecknit NC-Consil® 750 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Shielding Effectiveness | 100 dB @Frequency 1.00e+9 Hz |
100 dB @Frequency 1.00e+9 Hz |
Plane Wave |
Parker Chomerics Tecknit NC-Consil® 750 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Shielding Effectiveness | 100 dB @Frequency 100000 Hz |
100 dB @Frequency 100000 Hz |
H-Field |
Parker Chomerics Tecknit NC-Consil® 751 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Shielding Effectiveness | 100 dB @Frequency 1.00e+7 Hz |
100 dB @Frequency 1.00e+7 Hz |
E-Field |
Parker Chomerics Tecknit NC-Consil® 751 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Shielding Effectiveness | 100 dB @Frequency 1.00e+9 Hz |
100 dB @Frequency 1.00e+9 Hz |
Plane Wave |
Parker Chomerics Tecknit NC-Consil® 751 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Shielding Effectiveness | 100 dB @Frequency 1.00e+7 Hz |
100 dB @Frequency 1.00e+7 Hz |
E-Field |
Parker Chomerics Tecknit NC-Consil® 770 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Shielding Effectiveness | 100 dB @Frequency 1.00e+9 Hz |
100 dB @Frequency 1.00e+9 Hz |
Plane Wave |
Parker Chomerics Tecknit NC-Consil® 770 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 5.00e+8 Hz |
>= 100 dB @Frequency 5.00e+8 Hz |
E Field; CHO-TM-TP08 |
Parker Chomerics CHO-SEAL 1273 Conductive Elastomer Commercial Grade Conductive Elastomer Extrusions. These materials offer excellent cost/performance characteristics for commercial EMI gasket applications. These silicone and fluorosilicone based con.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 2.00e+9 Hz |
>= 100 dB @Frequency 2.00e+9 Hz |
Plane Wave; CHO-TM-TP08 |
Parker Chomerics CHO-SEAL 1273 Conductive Elastomer Commercial Grade Conductive Elastomer Extrusions. These materials offer excellent cost/performance characteristics for commercial EMI gasket applications. These silicone and fluorosilicone based con.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 1.00e+10 Hz |
>= 100 dB @Frequency 1.00e+10 Hz |
Plane Wave; CHO-TM-TP08 |
Parker Chomerics CHO-SEAL 1273 Conductive Elastomer Commercial Grade Conductive Elastomer Extrusions. These materials offer excellent cost/performance characteristics for commercial EMI gasket applications. These silicone and fluorosilicone based con.. |
|||
Shielding Effectiveness | 100 - 105 dB @Frequency 1.00e+9 - 2.00e+9 Hz |
100 - 105 dB @Frequency 1.00e+9 - 2.00e+9 Hz |
|
Master Bond MB600S Aqueous Based Sodium Silicate System for EMI/RFI Shielding Description: Master Bond MB600S is a silver containing aqueous based sodium silicate system used as a coating in situations where EMI shielding effectiveness is paramount. Electromagnetic interferen.. |