Physical Properties Metric English Comments
Specific Gravity 1.75 - 2.25 g/cc
1.75 - 2.25 g/cc
ASTM D792
Parker Chomerics CHO-SEAL 1285 Conductive Elastomer
Conductive Elastomer with Improved Corrosion Resistance. This conductive silicone elastomer features significantly improved corrosion resistance in salt spray environments over silver-plated copper-..
Specific Gravity 1.75 - 2.25 g/cc
1.75 - 2.25 g/cc
ASTM D792
Parker Chomerics CHO-SEAL 1287 Conductive Elastomer
Conductive Fluorosilicone EMI/EMP Gasket. This material is silver-plated-aluminum-filled fluorosilicone elastomer which provides pressure and environmental sealing as well as high levels of EMI shie..
Specific Gravity 1.75 - 2.25 g/cc
1.75 - 2.25 g/cc
ASTM D792
Parker Chomerics CHO-SEAL 1298 EMI Shielding Material
Corrosion Resistant EMI Shielding Gasket. Through the use of new proprietary particle painting and elastomer compounding technology, CHO-SEAL® 1298 shielding elastomer offers a six-fold increase in..
Specific Gravity 1.75 - 2.25 g/cc
1.75 - 2.25 g/cc
ASTM D792
Parker Chomerics CHO-SEAL S6305 Conductive Elastomer
Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Molded and Extruded.RoHS CompliantInformation provi..
Specific Gravity 1.75 - 2.25 g/cc
1.75 - 2.25 g/cc
ASTM D792
Parker Chomerics CHO-SEAL® 6308 Conductive Elastomer
Description: Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Extruded onlyRoHS CompliantInformation..
Specific Gravity 1.75 - 2.25 g/cc
1.75 - 2.25 g/cc
ASTM D792
Parker Chomerics CHO-SEAL® 6371 Conductive Elastomer
Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Molded onlyRoHS Compliant Information provided by C..
Specific Gravity 1.75 - 2.25 g/cc
1.75 - 2.25 g/cc
Base Material; ASTM D792
Parker Chomerics CHO-SEAL 1287R Reinforced Conductive Elastomer Seal
These materials are fabric-reinforced, silver-plated-aluminum filled EMI seals for airframe shielding applications. These seal materials can also be used to maintain surface electrical continuity at..
Specific Gravity 2.23 - 2.25 g/cc
2.23 - 2.25 g/cc
ASTM D792
Adamas Adalon® 237 PTFE, 25% Glass Fiber
Information provided by Adamas, HPM
Specific Gravity 1.75 - 2.25 g/cc
1.75 - 2.25 g/cc
Parker Chomerics CHO-BOND 1075 Silicone RTV Adhesive/Sealant
Electrically conductive, one component silicone adhesive/sealant that may be used for bonding EMI gaskets or for providing EMI and environmental protection as a caulk. This material cures on exposur..