Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Parker Chomerics CHO-SEAL 1287 Conductive Elastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Rubber or Thermoset Elastomer (TSE)
Manufacturer Parker Chomerics
Trade Name CHO-SEAL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-SEAL 1287 Conductive Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Conductive Fluorosilicone EMI/EMP Gasket. This material is silver-plated-aluminum-filled fluorosilicone elastomer which provides pressure and environmental sealing as well as high levels of EMI shielding. It is one of the more corrosion resistant silver-based elastomers, and is recommended where both salt spray and jet fuel environments are present.Molded and ExtrudedInformation provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 1.75 - 2.25 g/cc
1.75 - 2.25 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 63 - 77
63 - 77
ASTM D2240
Tensile Strength at Break >= 1.24 MPa
>= 180 psi
ASTM D412
Elongation at Break 60 - 260 %
60 - 260 %
ASTM D412
Tear Strength 6.13 kN/m
35.0 pli
ASTM D624
Compression Set <= 30 %

@Temperature 100 °C,
Time 252000 sec
<= 30 %

@Temperature 212 °F,
Time 70.0 hour
ASTM D395 Method B
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Flex TR10; ASTM D1329
Electrical Properties Metric English Comments
Volume Resistivity 0.012 ohm-cm
0.012 ohm-cm
without psa; MIL-DTL-83528
0.015 ohm-cm
0.015 ohm-cm
Post Tensile Set; MIL-G-83528 Para.4.6.9
Shielding Effectiveness >= 55 dB

@Frequency 200000 Hz
>= 55 dB

@Frequency 200000 Hz
H Field; MIL-DTL-83528 Para.4.6.12
>= 75 dB

@Frequency 4.00e+10 Hz
>= 75 dB

@Frequency 4.00e+10 Hz
Plane Wave; MIL-DTL-83528 Para.4.6.12
>= 90 dB

@Frequency 1.00e+10 Hz
>= 90 dB

@Frequency 1.00e+10 Hz
Plane Wave; MIL-DTL-83528 Para.4.6.12
>= 95 dB

@Frequency 2.00e+9 Hz
>= 95 dB

@Frequency 2.00e+9 Hz
Plane Wave; MIL-DTL-83528 Para.4.6.12
>= 100 dB

@Frequency 5.00e+8 Hz
>= 100 dB

@Frequency 5.00e+8 Hz
E Field; MIL-DTL-83528 Para.4.6.12
>= 110 dB

@Frequency 1.00e+8 Hz
>= 110 dB

@Frequency 1.00e+8 Hz
E Field; MIL-DTL-83528 Para.4.6.12
Descriptive Properties Value Comments
Binder Fluoro-silicone
EMP Survivability >0.9 kA / in
MIL-DTL-83528 Para.4.6.16
Filler Ag/Al
Grade Military-Aerospace
Heat Aging <0.015 ohm-cm
MIL-DTL-83528 Para.4.6.15
Type D
MIL-DTL-83528
Vibration Resistance, After <0.012 ohm-cm
MIL-DTL-83528 Para.4.6.13
Vibration Resistance, During <0.015 ohm-cm
MIL-DTL-83528 Para.4.6.13
Users viewing this material also viewed the following: