Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 95 dB @Frequency 4.00e+8 Hz |
95 dB @Frequency 4.00e+8 Hz |
P-Field |
P & P Technology Aluminum 5056 (AMS 4182) Knitted Cored Shielding Mesh Product has a diameter of 0.11mm.Information provided by P & P Technology |
|||
Shielding Effectiveness | 95 dB @Frequency 1.00e+8 Hz |
95 dB @Frequency 1.00e+8 Hz |
H-Field; Mil-G-83528/MIL std 285 |
P & P Technology Nickel Graphite Loaded EPDM Molding grade conductive EPDM elastomer loaded with nickel graphite filler. The material is dark grey in color and is specially compounded to give high EMC performance and excellent IP sealing.Infor.. |
|||
Shielding Effectiveness | 95 dB @Frequency 1.00e+9 Hz |
95 dB @Frequency 1.00e+9 Hz |
P-Field |
P & P Technology Oriented Wires In Silicone P & P Technology SP, SS, SR, SW & SF Ranges of gasket materials consist of Monel or aluminum wires embedded into solid silicone, sponge silicone or fluorosilicone, a fire retardant variant is also a.. |
|||
Shielding Effectiveness | >= 95 dB @Frequency 2.00e+9 Hz |
>= 95 dB @Frequency 2.00e+9 Hz |
Plane Wave; MIL-DTL-83528 Para.4.6.12 |
Parker Chomerics CHO-SEAL 1287 Conductive Elastomer Conductive Fluorosilicone EMI/EMP Gasket. This material is silver-plated-aluminum-filled fluorosilicone elastomer which provides pressure and environmental sealing as well as high levels of EMI shie.. |
|||
Shielding Effectiveness | >= 95 dB @Frequency 2.00e+9 Hz |
>= 95 dB @Frequency 2.00e+9 Hz |
Plane Wave; MIL-DTL-83528 Para.4.6.12 |
Parker Chomerics CHO-SEAL 1298 EMI Shielding Material Corrosion Resistant EMI Shielding Gasket. Through the use of new proprietary particle painting and elastomer compounding technology, CHO-SEAL® 1298 shielding elastomer offers a six-fold increase in.. |
|||
Shielding Effectiveness | >= 95 dB @Frequency 2.00e+9 Hz |
>= 95 dB @Frequency 2.00e+9 Hz |
Plane Wave; CHO-TM-TP08 |
Parker Chomerics CHO-SEAL 6370 Conductive Elastomer Commercial Grade Conductive Elastomer Extrusions. These materials offer excellent cost/performance characteristics for commercial EMI gasket applications. These silicone and fluorosilicone based con.. |
|||
Shielding Effectiveness | >= 95 dB @Frequency 1.00e+10 Hz |
>= 95 dB @Frequency 1.00e+10 Hz |
Plane Wave; CHO-TM-TP08 |
Parker Chomerics CHO-SEAL 6370 Conductive Elastomer Commercial Grade Conductive Elastomer Extrusions. These materials offer excellent cost/performance characteristics for commercial EMI gasket applications. These silicone and fluorosilicone based con.. |
|||
Shielding Effectiveness | >= 95 dB @Frequency 1.00e+8 Hz |
>= 95 dB @Frequency 1.00e+8 Hz |
E Field; Method 3, CHO-TM-TP09 |
Parker Chomerics CHO-SEAL® 6503 Conductive Elastomer Description: Highest performance in harsh environments; excellent shielding; best choice for corrosion requirements against aluminum.Molded and ExtrudedRoHS CompliantInformation provided by Chomeric.. |
|||
Shielding Effectiveness | >= 95 dB @Frequency 1.00e+8 Hz |
>= 95 dB @Frequency 1.00e+8 Hz |
E-Field; Method 2, MIL-DTL-83528 Para. 4.6.12 |
Parker Chomerics CHO-SEAL® 6307 Conductive Elastomer Description: Good performance in moderately corrosive environments; excellent NBC fluid resistance; good physical properties.Molded onlyRoHS CompliantInformation provided by Chomerics |
|||
Shielding Effectiveness | 95 dB @Frequency 1.00e+8 Hz |
95 dB @Frequency 1.00e+8 Hz |
|
Parker Chomerics SOFT-SHIELD® 2000 Low Closure Force, Foam Core EMI Gasket Description: SOFT-SHIELD® 2000 Series gaskets consist of silver-plated nylon yarn knitted as the outer layer over a highly compressible, thermoplastic EPDM foam core. Through a special treatment pr.. |
|||
Shielding Effectiveness | 95 dB @Frequency 2.00e+7 - 1.00e+10 Hz |
95 dB @Frequency 2.00e+7 - 1.00e+10 Hz |
CHO-TM-TP08 |
Parker Chomerics SOFT-SHIELD® 4850 Multi-planar EMI Gasket Description: SOFT-SHIELD® 4850 represents the latest advancement in EMI shielding gaskets based on Multi-planar, Z-axis conductive foam technology. SS4850 is based on the unique integration of elec.. |