Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 6.13 kN/m | 35.0 pli | ASTM D624 |
Parker Chomerics CHO-SEAL 1287 Conductive Elastomer Conductive Fluorosilicone EMI/EMP Gasket. This material is silver-plated-aluminum-filled fluorosilicone elastomer which provides pressure and environmental sealing as well as high levels of EMI shie.. |
|||
Tear Strength | 6.13 kN/m | 35.0 pli | ASTM D624 |
Parker Chomerics CHO-SEAL 1298 EMI Shielding Material Corrosion Resistant EMI Shielding Gasket. Through the use of new proprietary particle painting and elastomer compounding technology, CHO-SEAL® 1298 shielding elastomer offers a six-fold increase in.. |
|||
Tear Strength | 6.13 kN/m | 35.0 pli | ASTM D624 |
Parker Chomerics CHO-SEAL 6370 Conductive Elastomer Commercial Grade Conductive Elastomer Extrusions. These materials offer excellent cost/performance characteristics for commercial EMI gasket applications. These silicone and fluorosilicone based con.. |
|||
Tear Strength | 6.13 kN/m | 35.0 pli | ASTM D624 |
Parker Chomerics CHO-SEAL L6303 Conductive Elastomer Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Molded and ExtrudedRoHS CompliantInformation provid.. |
|||
Tear Strength | 6.13 kN/m | 35.0 pli | |
Parker Chomerics CHO-SEAL S6304 Conductive Elastomer Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics |
|||
Tear Strength | 6.13 kN/m | 35.0 pli | |
Parker Chomerics CHO-SEAL® 6315 Graphite Filled Elastomer EMI Gaskets. This extruded nickel-plated graphite filled elastomer addresses EMI shielding and environmental needs for both internal and external applications. It has an excellent performance in sal.. |
|||
Tear Strength | 6.13 kN/m | 35.0 pli | ASTM D624 |
Parker Chomerics CHO-SEAL 1217 Conductive Elastomer Resists highest level of EMP induced current; military gasket of choice in non-corrosive environments; excellent processing for molding and extrusion. Molded and ExtrudedRoHS Compliant Information p.. |