Material Notes:
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational demands.Information provided by PEAK Werkstoff GmbH
Physical Properties Metric English Comments
Density 2.413 - 2.667 g/cc
0.08718 - 0.09635 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers >= 65
>= 65
HV30
Tensile Strength at Break >= 128 MPa

@Temperature 150 °C
>= 18600 psi

@Temperature 302 °F
>= 165 MPa

@Temperature 20.0 °C
>= 23900 psi

@Temperature 68.0 °F
Tensile Strength, Yield >= 76.0 MPa

@Temperature 150 °C
>= 11000 psi

@Temperature 302 °F
>= 95.0 MPa

@Temperature 20.0 °C
>= 13800 psi

@Temperature 68.0 °F
Elongation at Break >= 2.5 %

@Temperature 20.0 °C
>= 2.5 %

@Temperature 68.0 °F
>= 8.4 %

@Temperature 150 °C
>= 8.4 %

@Temperature 302 °F
Modulus of Elasticity >= 76.0 GPa

@Temperature 150 °C
>= 11000 ksi

@Temperature 302 °F
>= 85.0 GPa

@Temperature 20.0 °C
>= 12300 ksi

@Temperature 68.0 °F
Poissons Ratio 0.275

@Temperature 20.0 °C
0.275

@Temperature 68.0 °F
0.278

@Temperature 100 °C
0.278

@Temperature 212 °F
0.28

@Temperature 150 °C
0.28

@Temperature 302 °F
0.282

@Temperature 200 °C
0.282

@Temperature 392 °F
0.284

@Temperature 250 °C
0.284

@Temperature 482 °F
0.284

@Temperature 300 °C
0.284

@Temperature 572 °F
Shear Modulus 33.0 GPa

@Temperature 250 °C
4790 ksi

@Temperature 482 °F
33.0 GPa

@Temperature 300 °C
4790 ksi

@Temperature 572 °F
34.0 GPa

@Temperature 200 °C
4930 ksi

@Temperature 392 °F
35.0 GPa

@Temperature 100 °C
5080 ksi

@Temperature 212 °F
35.0 GPa

@Temperature 150 °C
5080 ksi

@Temperature 302 °F
36.0 GPa

@Temperature 20.0 °C
5220 ksi

@Temperature 68.0 °F
Thermal Properties Metric English Comments
CTE, linear 14.6 - 15.6 µm/m-°C

@Temperature 20.0 - 100 °C
8.11 - 8.67 µin/in-°F

@Temperature 68.0 - 212 °F
15.5 - 16.5 µm/m-°C

@Temperature 20.0 - 200 °C
8.61 - 9.17 µin/in-°F

@Temperature 68.0 - 392 °F
16.3 - 17.3 µm/m-°C

@Temperature 20.0 - 300 °C
9.06 - 9.61 µin/in-°F

@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.830 - 0.870 J/g-°C
0.198 - 0.208 BTU/lb-°F
Thermal Conductivity 123.5 W/m-K

@Temperature 400 °C
857.1 BTU-in/hr-ft²-°F

@Temperature 752 °F
131 W/m-K

@Temperature 300 °C
909 BTU-in/hr-ft²-°F

@Temperature 572 °F
136.8 W/m-K

@Temperature 200 °C
949.4 BTU-in/hr-ft²-°F

@Temperature 392 °F
144.3 W/m-K

@Temperature 100 °C
1001 BTU-in/hr-ft²-°F

@Temperature 212 °F
152.4 W/m-K

@Temperature 30.0 °C
1058 BTU-in/hr-ft²-°F

@Temperature 86.0 °F
Melting Point 573 - 881 °C
1060 - 1620 °F
Solidus 572.9 - 578.9 °C
1063 - 1074 °F
Liquidus 875.3 - 881.3 °C
1608 - 1618 °F
Component Elements Properties Metric English Comments
Aluminum, Al 65 %
65 %
As Balance
Silicon, Si 35 %
35 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000620 - 0.00000660 ohm-cm
0.00000620 - 0.00000660 ohm-cm