Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.830 - 0.870 J/g-°C | 0.198 - 0.208 BTU/lb-°F | |
PEAK Werkstoff DISPAL S220 Aluminum Alloy, AlSi35, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Specific Heat Capacity | 0.830 - 0.870 J/g-°C | 0.198 - 0.208 BTU/lb-°F | |
PEAK Werkstoff DISPAL S220 Aluminum Alloy, AlSi35, Condition O Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |