Mechanical Properties Metric English Comments
Tensile Strength at Break >= 165 MPa

@Temperature 20.0 °C
>= 23900 psi

@Temperature 68.0 °F
PEAK Werkstoff DISPAL S220 Aluminum Alloy, AlSi35, Condition F
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
Tensile Strength at Break 165 MPa

@Temperature 23.0 °C
23900 psi

@Temperature 73.4 °F
LATI Larton GCE/600 PPS, Glass/Mineral Reinforced
Polyphenylene Sulfide (PPS) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa ..
Tensile Strength at Break 165 MPa

@Temperature 23.0 °C
23900 psi

@Temperature 73.4 °F
LATI Larton GCE/650 PPS, Glass/Mineral Reinforced
Polyphenylene Sulfide (PPS) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa ..
Tensile Strength at Break 165 MPa

@Temperature 60.0 °C
23900 psi

@Temperature 140 °F
LATI Latamid 6 H2 G/55 PA 6, 55% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla..
Tensile Strength at Break 165 MPa

@Temperature 23.0 °C
23900 psi

@Temperature 73.4 °F
LATI Latamid SP1 G/30 PA 6.10, 30% Glass Fiber Reinforced
Polyamide 6.10 (PA6.10) based compound. Glass fibers. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus..
Tensile Strength at Break 165 MPa

@Temperature 120 °C
23900 psi

@Temperature 248 °F
LATI Laramid G/60 PPA, 60% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Tensile Strength at Break 165 MPa

@Temperature 60.0 °C
23900 psi

@Temperature 140 °F
LATI Larpeek 10 G/30 PEEK, 30% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Strength at Break 165 MPa

@Temperature 60.0 °C
23900 psi

@Temperature 140 °F
LATI Larton K/30 PPS, 30% Carbon Fiber Reinforced
Polyphenylene Sulfide (PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Strength at Break 165 MPa

@Temperature 23.0 °C
23900 psi

@Temperature 73.4 °F
ISO 527
BASF Ultramid® KR 4357 G6 30% Glass Filled PA6/6T (Dry)
Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan..
Tensile Strength at Break 165 MPa

@Temperature 23.0 °C
23900 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612  (Unverified Data**)
Zytel® 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Strength at Break 165 MPa

@Temperature 23.0 °C
23900 psi

@Temperature 73.4 °F
ISO 527-1
Vyncolit Neopreg Kinel® SK4502 S8 Carbon Reinforced Molding Compound
KINEL SK4502 S8 is a long carbon fiber reinforced BMI molding compound suited for very demanding tribological applications, high speeds and temperatures even under dry running conditions. Thermal ex..