Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.830 J/g-°C | 0.198 BTU/lb-°F | calculated |
Rogers Corporation TMM® TMM4 Ceramic Thermoset Polymer Composite TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope.. |
|||
Specific Heat Capacity | 0.830 - 0.870 J/g-°C | 0.198 - 0.208 BTU/lb-°F | |
PEAK Werkstoff DISPAL S220 Aluminum Alloy, AlSi35, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Specific Heat Capacity | 0.830 - 0.870 J/g-°C | 0.198 - 0.208 BTU/lb-°F | |
PEAK Werkstoff DISPAL S220 Aluminum Alloy, AlSi35, Condition O Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Specific Heat Capacity | 0.830 J/g-°C @Temperature 20.0 - 100 °C |
0.198 BTU/lb-°F @Temperature 68.0 - 212 °F |
|
Schott Nextrema® 712-3 Glass Ceramic The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal.. |
|||
Specific Heat Capacity | 0.830 J/g-°C @Temperature 20.0 - 100 °C |
0.198 BTU/lb-°F @Temperature 68.0 - 212 °F |
|
Schott Nextrema® 712-8 Glass Ceramic The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal.. |
|||
Specific Heat Capacity | 0.830 J/g-°C @Temperature 20.0 - 100 °C |
0.198 BTU/lb-°F @Temperature 68.0 - 212 °F |
|
Schott BOROFLOAT® Borosilicate Float Glass This is a highly chemically resistant borosilicate glass with a low thermal expansion. BOROFLOAT® replaced TEMPAX®, a drawn flat borosilicate glass for Schott. The high quality resulting fro.. |
|||
Specific Heat Capacity | 0.830 J/g-°C | 0.198 BTU/lb-°F | |
Schott N-KZFS2 Glass Information Provided by SCHOTT North America, Inc. |