Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | >= 85.0 GPa @Temperature 20.0 °C |
>= 12300 ksi @Temperature 68.0 °F |
|
PEAK Werkstoff DISPAL S220 Aluminum Alloy, AlSi35, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Modulus of Elasticity | >= 85.0 GPa @Temperature 20.0 °C |
>= 12300 ksi @Temperature 68.0 °F |
|
PEAK Werkstoff DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |