Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000620 - 0.00000660 ohm-cm | 0.00000620 - 0.00000660 ohm-cm | |
PEAK Werkstoff DISPAL S220 Aluminum Alloy, AlSi35, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Electrical Resistivity | 0.00000620 - 0.00000660 ohm-cm | 0.00000620 - 0.00000660 ohm-cm | |
PEAK Werkstoff DISPAL S220 Aluminum Alloy, AlSi35, Condition O Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |