Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 14.6 - 15.6 µm/m-°C @Temperature 20.0 - 100 °C |
8.11 - 8.67 µin/in-°F @Temperature 68.0 - 212 °F |
|
PEAK Werkstoff DISPAL S220 Aluminum Alloy, AlSi35, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
CTE, linear | 14.6 - 15.6 µm/m-°C @Temperature 20.0 - 100 °C |
8.11 - 8.67 µin/in-°F @Temperature 68.0 - 212 °F |
|
PEAK Werkstoff DISPAL S220 Aluminum Alloy, AlSi35, Condition O Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
CTE, linear | 14.6 - 15.6 µm/m-°C @Temperature 20.0 - 100 °C |
8.11 - 8.67 µin/in-°F @Temperature 68.0 - 212 °F |
|
PEAK Werkstoff DISPAL S225 Aluminum Alloy, AlSi35Fe2Ni, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |