Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000620 - 0.00000660 ohm-cm | 0.00000620 - 0.00000660 ohm-cm | |
PEAK Werkstoff DISPAL S220 Aluminum Alloy, AlSi35, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Electrical Resistivity | 0.00000620 - 0.00000660 ohm-cm | 0.00000620 - 0.00000660 ohm-cm | |
PEAK Werkstoff DISPAL S220 Aluminum Alloy, AlSi35, Condition O Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Electrical Resistivity | 0.00000580 - 0.00000660 ohm-cm | 0.00000580 - 0.00000660 ohm-cm | |
Constellium Alumold® 110 Aluminum Cast Sliced Plate Alumold®-110 has been specifically developed for low–pressure processing (thermoforming, RTM) of plastics and their composites. The material can also be used for prototype injection moulds. The ma.. |
|||
Electrical Resistivity | 0.00000590 - 0.00000660 ohm-cm | 0.00000590 - 0.00000660 ohm-cm | |
Constellium Fibral® Cast Aluminum Sliced Plate Fibral® has been specifically developed for low–pressure processing (thermoforming, RTM) of plastics and their composites. The material can also be used for prototype injection moulds. The materia.. |
|||
Electrical Resistivity | 0.00000590 - 0.00000660 ohm-cm | 0.00000590 - 0.00000660 ohm-cm | |
Constellium Formall® 545 Aluminum Alloy Formall®-545 is a super plastically formable alloy. Both chemical composition and processing conditions have been developed for optimum superplastic behavior and to guarantee the advantages of an a.. |
|||
Electrical Resistivity | 0.00000580 - 0.00000660 ohm-cm | 0.00000580 - 0.00000660 ohm-cm | |
Constellium PLAN 5083 Aluminum Rolled Plate Rolled plates in 5083 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 5083 PLAN is mainly used for low stressed mechanical components, manufactured by intensive m.. |
|||
Electrical Resistivity | 0.00000590 - 0.00000660 ohm-cm | 0.00000590 - 0.00000660 ohm-cm | |
Constellium Planoxal® 50 Aluminum plate Planoxal®-50 plates differ from other standard EN-AW 5083 alloy products by their low level of residual stress. This specialty plate is also suitable for decorative anodizing. Planoxal®-50 is main.. |
|||
Electrical Resistivity | 0.00000580 - 0.00000660 ohm-cm | 0.00000580 - 0.00000660 ohm-cm | |
Constellium ALPLAN® 5083 Rolled Precision Aluminum Plate, Milled Both Sides ALPLAN® 5083 precision plates exhibit good dimensional stability. Their low internal stresses reduces the effects of plate deformation during machining, thus saving on extra operations such as roug.. |