Polymer Property : CTE, linear = 15.6 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 14.6 - 15.6 µm/m-°C

@Temperature 20.0 - 100 °C
8.11 - 8.67 µin/in-°F

@Temperature 68.0 - 212 °F
PEAK Werkstoff DISPAL S220 Aluminum Alloy, AlSi35, Condition F
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
CTE, linear 14.6 - 15.6 µm/m-°C

@Temperature 20.0 - 100 °C
8.11 - 8.67 µin/in-°F

@Temperature 68.0 - 212 °F
PEAK Werkstoff DISPAL S220 Aluminum Alloy, AlSi35, Condition O
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
CTE, linear 14.6 - 15.6 µm/m-°C

@Temperature 20.0 - 100 °C
8.11 - 8.67 µin/in-°F

@Temperature 68.0 - 212 °F
PEAK Werkstoff DISPAL S225 Aluminum Alloy, AlSi35Fe2Ni, Condition F
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..