Overview of materials for Nylon 11, Flexible Tubing Grade

Category Polymer , Thermoplastic , Nylon , Nylon 11 , Nylon 11, Flexible Tubing Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Nylon 11, Flexible Tubing Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Flexible Tubing Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.00 - 1.08 g/cc
0.0361 - 0.0390 lb/in³
Average value: 1.04 g/cc Grade Count:12
Water Absorption 1.30 - 1.80 %
1.30 - 1.80 %
Average value: 1.52 % Grade Count:5
Melt Flow 1.00 - 15.5 g/10 min
1.00 - 15.5 g/10 min
Average value: 6.43 g/10 min Grade Count:14
Mechanical Properties Metric English Comments
Tensile Strength, Yield 15.0 - 33.0 MPa
2180 - 4790 psi
Average value: 25.1 MPa Grade Count:14
Elongation at Break 50.0 %
50.0 %
Average value: 50.0 % Grade Count:14
Elongation at Yield 20.0 - 38.0 %
20.0 - 38.0 %
Average value: 30.5 % Grade Count:8
Modulus of Elasticity 0.165 - 0.610 GPa
23.9 - 88.5 ksi
Average value: 0.399 GPa Grade Count:14
Charpy Impact Unnotched NB
NB
Grade Count:10
Charpy Impact, Notched 3.80 J/cm² - NB
18.1 ft-lb/in² - NB
Average value: 4.65 J/cm² Grade Count:10
0.330 - 1.22 J/cm²

@Temperature -30.0 - -30.0 °C
1.57 - 5.81 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.726 J/cm² Grade Count:10
Thermal Properties Metric English Comments
CTE, linear 90.0 - 150 µm/m-°C
50.0 - 83.3 µin/in-°F
Average value: 113 µm/m-°C Grade Count:7
Melting Point 150 - 183 °C
302 - 361 °F
Average value: 172 °C Grade Count:12
Deflection Temperature at 0.46 MPa (66 psi) 69.0 - 147 °C
156 - 297 °F
Average value: 111 °C Grade Count:5
Deflection Temperature at 1.8 MPa (264 psi) 36.0 - 55.0 °C
96.8 - 131 °F
Average value: 43.1 °C Grade Count:7
Vicat Softening Point 95.0 - 180 °C
203 - 356 °F
Average value: 146 °C Grade Count:6
Flammability, UL94 HB - V-2
HB - V-2
Grade Count:12
Optical Properties Metric English Comments
Transmission, Visible 80.0 %
80.0 %
Average value: 80.0 % Grade Count:4
Electrical Properties Metric English Comments
Electrical Resistivity 5.00e+9 - 1.00e+12 ohm-cm
5.00e+9 - 1.00e+12 ohm-cm
Average value: 4.33e+11 ohm-cm Grade Count:5
Surface Resistance 5.00e+11 - 4.00e+14 ohm
5.00e+11 - 4.00e+14 ohm
Average value: 1.11e+14 ohm Grade Count:4
Dielectric Strength 18.0 - 34.0 kV/mm
457 - 864 kV/in
Average value: 26.2 kV/mm Grade Count:5