Physical Properties Metric English Comments
Density 1.08 - 1.08 g/cc

@Temperature 285 - 285 °C
0.0390 - 0.0390 lb/in³

@Temperature 545 - 545 °F
Average value: 1.08 g/cc Grade Count:2
Overview of materials for PCTG Copolyester
This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M..
Density 1.08 - 1.08 g/cc

@Temperature 300 - 300 °C
0.0390 - 0.0390 lb/in³

@Temperature 572 - 572 °F
Average value: 1.08 g/cc Grade Count:5
Overview of materials for Polycarbonate, 10% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea..
Density 1.00 - 1.08 g/cc
0.0361 - 0.0390 lb/in³
Average value: 1.04 g/cc Grade Count:12
Overview of materials for Nylon 11, Flexible Tubing Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Flexible Tubing Grade". Each property range of values reported is minimum and maximum values o..
Density 1.02 - 1.08 g/cc
0.0368 - 0.0390 lb/in³
Average value: 1.05 g/cc Grade Count:5
Overview of materials for Nylon 12, Graphite Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Graphite Filled". Each property range of values reported is minimum and maximum values of appr..
Density 1.03 - 1.08 g/cc
0.0372 - 0.0390 lb/in³
Lord Adhesives 206 Long Working Time Acrylic Adhesive
Lord 200 SeriesLord 200 Series Acrylic Adhesives bond minimally prepared or unprepared surfaces. They offer excellent adhesion to unprepared metals, ceramic magnets and plastics. Viscosities range f..
Density 1.07 - 1.08 g/cc
0.0387 - 0.0390 lb/in³
Guarniflon TENFIL TF 200 Polytetrafluoroethylene Thread Sealant
TENFIL TF200 is a PTFE-based thread sealant in water dispersion, which increases the tightness of the threaded parts and prevents leakage of water. The product is intended for the assembly of fitti..
Density 1.02 - 1.08 g/cc
0.0368 - 0.0390 lb/in³
ASTM D 792
Karina E 5525/1-TRE Kariprene Natural.
Thermoplastic rubber compound, recommended for injection of footwear soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Density 1.04 - 1.08 g/cc
0.0376 - 0.0390 lb/in³
Shandong Guangyin PA 612 Nylon Resin
Features and Applications: As one kind of nylon with better tenacity, PA612 is mainly applicable to coating of high-grade toothbrush monofilaments, monofilaments and cables.Information provided by S..
Density 0.959 - 1.08 g/cc
0.0346 - 0.0390 lb/in³
3M 1000NF Fast Tack Water Based Adhesive
3M™ Fast Tack Water Based Adhesive 1000NF is a high performance water-based, one part adhesive formulated for fast bonding and long term heat resistant bonds.Information provided by 3M
Density 1.04 - 1.08 g/cc
0.0376 - 0.0390 lb/in³
ISO 1183
Austin Novel Materials Texalan® 565A Polyether-based TPU
Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech
Density 1.01 - 1.08 g/cc
0.0365 - 0.0390 lb/in³
3M 32665 Green Heavy Duty Performance Coating - Part B
3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and ..
Density 1.01 - 1.08 g/cc
0.0365 - 0.0390 lb/in³
3M 32666 Tan Heavy Duty Performance Coating - Part B
3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and ..
Density 1.04 - 1.08 g/cc
0.0376 - 0.0390 lb/in³
ISO 1183
Austin Novel Materials Texalan® 570A Polyether-based TPU
Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech
Density 1.01 - 1.08 g/cc
0.0365 - 0.0390 lb/in³
3M 32663 Medium Grey Heavy Duty Performance Coating - Part B
3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and ..
Density 1.01 - 1.08 g/cc
0.0365 - 0.0390 lb/in³
3M 32664 Light Gray Heavy Duty Performance Coating - Part B
3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and ..