Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.165 - 0.610 GPa | 23.9 - 88.5 ksi | Average value: 0.399 GPa Grade Count:14 |
Overview of materials for Nylon 11, Flexible Tubing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Flexible Tubing Grade". Each property range of values reported is minimum and maximum values o.. |