Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 150 °C | 302 °F | |
Plastcom SLOVALEN PC 51 T 25 PP, 25% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 25% microground, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitu.. |
|||
Melting Point | 150 °C | 302 °F | DSC; STN EN ISO 3146 |
Plastcom SLOVALEN PC 78 FRD 1 Polypropylene Copolymer, Halogen Flame Retardant, UV Stabilized FeaturesModified copolymer PP with the possibility of changing the MFI within the interval 5 - 20 g/10min. Stabilized against the UV-radiation by the UV stabilizer on the HALS basis. Retarded with.. |
|||
Melting Point | 150 °C | 302 °F | DSC; STN EN ISO 3146 |
Plastcom SLOVALEN PC 78 FRD 3 Polypropylene Copolymer, Halogen Flame Retardant FeaturesDetermined for environment where contact with water is possible because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machine.. |
|||
Melting Point | 150 °C | 302 °F | |
Plastcom SLOVALEN PH 91 N PP, basic type FeaturesCompounded homopolymer PP. General use in all industry branches. Packing material, garden flower-pots, toys, furniture industry, guides, dowels, clamps, office chairs, holders etc. Delivered.. |
|||
Melting Point | 150 °C | 302 °F | Flow temperature, ASTM D569-59 |
Rotuba 855, Slow Burning Ethyl Cellulose Data provided by the manufacturer. |
|||
Melting Point | 150 °C | 302 °F | DSC second heating; ASTM D3418 |
Reliance Industries Repol R110MK Polypropylene REPOL Polypropylene R110MK is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Melting Point | 150 °C | 302 °F | DSC second heating; ASTM D3418 |
Reliance Industries Repol R120MK Polypropylene REPOL Polypropylene R120MK is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Melting Point | 150 °C | 302 °F | Flow temperature, ASTM D569 |
Rotuba MH Cellulose Acetate Property values at 50% RH.Data provided by the manufacturer. |
|||
Melting Point | 150 - 160 °C | 302 - 320 °F | ASTM D3418 |
NatureWorks® Ingeo™ 6752D Spunbond Grade Biopolymer Sheath polymer for spunbound uses. NatureWorks® PLA polymer 6752D, a NatureWorks LLC product, is a thermoplastic fiber-grade resin de-rived from annually renewable resources. Available in pellet f.. |
|||
Melting Point | 150 - 182 °C | 302 - 360 °F | Average value: 164 °C Grade Count:5 |
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |
|||
Melting Point | 150 - 170 °C | 302 - 338 °F | ISO 3146-C |
FKuR Kunststoff Bio-Flex® F 6611 Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Melting Point | 150 - 170 °C | 302 - 338 °F | ISO 3146-C |
FKuR Kunststoff Bio-Flex® S 9533 Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Melting Point | 150 - 160 °C | 302 - 320 °F | ISO 3146-C |
FKuR Kunststoff Fibrolon® F 8530 Biodegradable Wood-Plastic Compound, Fiber Reinforced FIBROLON® are fiber reinforced compounds. Depending on specific customer requirements either a biodegradable polymer or a polyolefin can be used as the polymeric matrix. With the brand name of F.. |
|||
Melting Point | 150 - 180 °C | 302 - 356 °F | ISO 3146-C |
FKuR Kunststoff Fibrolon® P 7550 Wood-Plastic Compound, Fiber Reinforced FIBROLON® are fiber reinforced compounds. Fibrolon® P 7550 has a polypropylene base. With the brand name of FIBROLON® FKuR has developed natural fiber reinforced compounds (Wood-Plastics-C.. |
|||
Melting Point | 150 °C | 302 °F | Peak |
LG Chemical KEYFLEX BT 3140D Ester Type TPE Description: Injection Molding, TPC-ET, Specialty, Low Melting Temperature, Low ModulusApplication: Masterbatch Carrier, Cable Compound BaseCAS: 37282-12-5Information provided by LG Chemical |
|||
Melting Point | 150 °C | 302 °F | |
Indium Corp. Indalloy 88 Indium Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 150 °C | 302 °F | |
LG Chemical NBR 7030S High Acrylonitrile Polymer Description: NBR 7030S has combined the merit of NBR (Acrylonitrile rubber) with the merit of PVC resin. NBR 7030S shows good flexibility and elasticity without vulcanization, and also shows good oi.. |
|||
Melting Point | 150 - 200 °C | 302 - 392 °F | |
LG Chemical SEETEC BC500 LDPE Good Processability and Good electrical properties. Main Application: Cable insulationCAS No. 9002-88-4Information provided by LG Chemical |
|||
Melting Point | 150 - 350 °C | 302 - 662 °F | |
Johnson Matthey JM A-Core Soft Solder Flux The standard "acid" flux core used for most industrial applications where an aggressive flux is required. Residues are corrosive.Information provided by Johnson Matthey. |
|||
Melting Point | 150 - 350 °C | 302 - 662 °F | |
Johnson Matthey JM No1S Soft Solder Flux A highly active liquid flux recommended for use on Stainless and carbon steels. Generally used with the Silver/Tin alloys such as JM P40 and JM P5. Residues are corrosive and should be removed aft.. |
|||
Melting Point | 150 - 300 °C | 302 - 572 °F | |
Johnson Matthey JM No2S Soft Solder Flux A liquid non-corrosive flux for use on copper and brass. The residues are water soluble and non-corrosive, however it is recommended they are removed to prevent any possibility of contamination aft.. |
|||
Melting Point | <= 150 °C | <= 302 °F | |
Struktol CALCIUM STEARATE High purity, non-wettable, calcium stearate powder manufactured with high quality stearic acid.STRUKTOL® Calcium Stearate is used by the rubber and plastic industries as an effective elastomer pr.. |
|||
Melting Point | 150 °C | 302 °F | ASTM D2117 |
SCG Chemicals EL-Proâ„¢ P852J Polypropylene Injection Molding Key Characteristics:Excellent productivityHigh clarityHigh stiffnessRecommended Applications:Clear food containerClear large size containerHousehold products and other articles that require high tra.. |
|||
Melting Point | 150 °C | 302 °F | DSC |
Total PPH M3661 Metallocene Isostatic Polypropylene Polymer, Cast Film Extrusion TOTAL Petrochemicals Polypropylene M3661 is an isostatic form of homopolymer made via TOTAL proprietary metallocene catalyst technologyRecommended Applications. M3661 is a medium molecular weight m.. |
|||
Melting Point | 150 °C | 302 °F | ASTM D3418, ISO 3146 |
DuPont™ Bynel® 50E662 Anhydride Modified Polypropylene BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen.. |
|||
Melting Point | 150 °C | 302 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Hytrel® 4053FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Melting Point | 150 °C | 302 °F | 10°C/min |
Arkema Group Rilsan® 6733 Nylon 11, Flexible Tubing Grade (Dry) Designation ISO 1874-PA11/xx,E,18-002Transparent and flexible copolymer for tubes extrusion. Additive free.High flexibility. Very good transparency. High chemical resistance.USP XXIII class VI appro.. |
|||
Melting Point | 150 - 170 °C | 302 - 338 °F | Average value: 164 °C Grade Count:14 |
Overview of materials for Polypropylene Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Melting Point | 150 - 182 °C | 302 - 360 °F | Average value: 159 °C Grade Count:19 |
Overview of materials for Polypropylene with 40% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are.. |
|||
Melting Point | 150 °C | 302 °F | ASTM D2117 |
Lushan PR320 Adhesive Resin for Aluminum Plastic Composite Pipe Adhesive resin Lushan series for aluminum-plastic composite pipe is maleic grafted polyethylene used for PE-AL-PE, PEX-AL-PEX and PERT-AL-PERT composite pipes. Lushan adhesive resin could provides i.. |