Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact, Notched = 0.330 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.330 J/cm²

@Temperature -30.0 °C
1.57 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Nilit FRIANYL A63 HH-KV20 Nylon 6.6 for injection molding, 20% glass ball reinforced
Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact, Notched 0.330 J/cm²
1.57 ft-lb/in²
ISO 179/1eA
Solvay Specialty Polymers Amodel® A-1340 HS Polyphthalamide (PPA) Resin, 40% Mineral/Glass Reinforced, Dry as Molded &a
AMODEL® A-1340 HS is a 40% mineral/glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, high tensile strength and low warpage..
Charpy Impact, Notched 0.330 J/cm²

@Temperature -30.0 °C
1.57 ft-lb/in²

@Temperature -22.0 °F
Eastman Tenite 264-10 CAB Cellulose Acetate Butyrate  (discontinued **)
10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical.
Charpy Impact, Notched 0.330 - 1.22 J/cm²

@Temperature -30.0 - -30.0 °C
1.57 - 5.81 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.726 J/cm² Grade Count:10
Overview of materials for Nylon 11, Flexible Tubing Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Flexible Tubing Grade". Each property range of values reported is minimum and maximum values o..
Charpy Impact, Notched 0.330 J/cm²

@Temperature 23.0 °C
1.57 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/1eA
FKuR Kunststoff Fibrolon® P 7550 Wood-Plastic Compound, Fiber Reinforced
FIBROLON® are fiber reinforced compounds. Fibrolon® P 7550 has a polypropylene base. With the brand name of FIBROLON® FKuR has developed natural fiber reinforced compounds (Wood-Plastics-C..
Charpy Impact, Notched 0.330 J/cm²

@Temperature 23.0 °C
1.57 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1A
Gromax BFM30-EL03N1 Nylon 6 30% Mineral Filled (Dry)
Information provided by Gromax Enterprises Corp.
Charpy Impact, Notched 0.330 J/cm²

@Temperature -20.0 °C
1.57 ft-lb/in²

@Temperature -4.00 °F
DIN 53453
Global PP-2300-NC Polypropylene Block Copolymer
Description-opacity, medium to high stiffness, high impact strength at low temperatureApplications-furniture, crates, closures, electrical appliances, automotiveInformation provided by Global Polyme..
Charpy Impact, Notched 0.330 J/cm²
1.57 ft-lb/in²
LATI Latishield 66-10A PA66, Steel Fiber Reinforced
EMI shielding product based on Polyamide 66 (PA66). Steel fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl..
Charpy Impact, Notched 0.330 J/cm²
1.57 ft-lb/in²
ISO 179/1eA
Polyplastics Duracon® TR-10D Acetal Co-polymer (POM), Mineral filling, Mineral filling, High rigidity, Low warpage
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
Charpy Impact, Notched 0.330 J/cm²
1.57 ft-lb/in²
ISO 179-1
Vyncolit BXE7670 Glass Filled Phenolic Molding Compound
Novolac resin based, mainly glass fiber filled. Due to its unique composition, excellent balance between mechanical, thermal and dimensional stability.Information provided by Sumitomo Bak North Ame..
Charpy Impact, Notched 0.330 J/cm²

@Temperature -30.0 °C
1.57 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
DuPont Performance Polymers Crastin® S650FR NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)<
Unreinforced Flame Retardant Polybutylene Terephthalate Crastin S650FR is an unreinforced flame retardant polybutylene terephthalate for injection molding.Information provided by DuPont Performance ..
Charpy Impact, Notched 0.330 J/cm²

@Temperature 23.0 °C
1.57 ft-lb/in²

@Temperature 73.4 °F
EN ISO 179
Ensinger TECASINT 1011 Polyimide (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
Charpy Impact, Notched 0.330 J/cm²

@Temperature 23.0 °C
1.57 ft-lb/in²

@Temperature 73.4 °F
EN ISO 179
Ensinger TECASINT™ 2031 Polyimide, 40% Graphite Filled (PI)
TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications...
Charpy Impact, Notched 0.330 J/cm²

@Temperature -30.0 °C
1.57 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® BESN F15 TL Nylon 11, Flexible Tubing Grade (Conditioned)
Designation ISO 1874-PA11-P,EHL,16-001High flexible grade for tubes extrusion. Available color: black and natural. Light and heat stabilized.High flexibility. High burst pressure and impact strength..
Charpy Impact, Notched 0.330 J/cm²
1.57 ft-lb/in²
ASTM D256
Chang Chun Plastic Longlite PM T373J Electrical Phenolic Molding Compound
ASTM Grades per ASTM D700 are 2, 3.Information provided by Dowell Trading Company Ltd.
Charpy Impact, Notched 0.330 - 0.740 J/cm²

@Temperature -30.0 - -30.0 °C
1.57 - 3.52 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.497 J/cm² Grade Count:3
Overview of materials for Cellulose Acetate Butyrate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Butyrate, Molded". Each property range of values reported is minimum and maximum value..
Copyright © lookpolymers.com All Rights Reserved