Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nilit FRIANYL A63 W-GV15 Nylon 6.6 for injection molding, 15% glass fiber reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 20% Glass Fiber Filled
Manufacturer Nilit (formerly Frisetta Polymer)
Trade Name FRIANYL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nilit FRIANYL A63 W-GV15 Nylon 6.6 for injection molding, 15% glass fiber reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ISO 1183
Water Absorption 1.5 - 2.2 %
1.5 - 2.2 %
ISO 62
Water Absorption at Saturation 6.0 - 8.0 %
6.0 - 8.0 %
ISO 62
Viscosity Measurement 145
145
Viscosity index; ISO 307
Linear Mold Shrinkage 0.0050 - 0.022 cm/cm
0.0050 - 0.022 in/in
FRISETTA Test Method
Mechanical Properties Metric English Comments
Ball Indentation Hardness 170 MPa
24700 psi
ISO 2039-1
Tensile Strength at Break 140 MPa
20300 psi
ISO 527
Elongation at Break 5.0 %
5.0 %
ISO 527
Tensile Modulus 6.00 GPa
870 ksi
ISO 527
Flexural Strength 170 MPa
24700 psi
ISO 178
Flexural Modulus 5.60 GPa
812 ksi
ISO 178
Charpy Impact Unnotched 3.00 J/cm²
14.3 ft-lb/in²
DIN 53453
2.50 J/cm²

@Temperature -40.0 °C
11.9 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
DIN 53453
Thermal Properties Metric English Comments
Melting Point 256 °C
493 °F
ISO 3146 DSC
Maximum Service Temperature, Air 115 °C
239 °F
Continuous; FRISETTA Test Method
Deflection Temperature at 0.46 MPa (66 psi) 250 °C
482 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
ISO 75
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 93
Dissipation Factor 0.020

@Frequency 1e+6 Hz
0.020

@Frequency 1e+6 Hz
IEC 250
Comparative Tracking Index 550 V
550 V
CTI 100; IEC 112
Copyright © lookpolymers.com All Rights Reserved