Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.23 g/cc | 0.0444 lb/in³ | ISO 1183 |
Nilit FRIANYL A63 H-GV15 Nylon 6.6 for injection molding, 15% glass fiber reinforced Nylon 6.6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ASTM D792 |
PTS Tristar® PC-10FRNH 12 MFI Non-Bromine Non-Chlorine Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | DIN 53479; ASTM D792 |
Kolon KOPEL® KP3363 General Purpose TPE Resin KOPEL® is a thermoplastic polyester elastomer which is a new engineering rubber having combined properties of conventional rubber and thermoplastic. Its flexibility and elastic recovery are very.. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ASTM D792B |
LyondellBasell Astryn BE17FC Polypropylene Copolymer, 40% Calcium Carbonate Key Features: fractional melt flow, medium high modulus, UV-stabilized, mineral-filled, blow molding and extrusion grade polypropylene copolymer, excellent impact and stiffness balance, good melt st.. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP DX96651 PC LNP LUBRICOMP* DX96651 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 GF/B20 A2 20% Glass Fiber/Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber/Glass Bead, 20% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedInformation .. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6/6 CM16 HS BK 16% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 16% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackInformation provided by TP Compo.. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6/6 GF13 X BK 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by Weight Additive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedAppearan.. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ASTM D792 |
Techmer ES HiFill® PP GF/M40 CC BK 40% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 40% Filler by WeightFeatures: Chemically CoupledAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ASTM D792 |
Techmer ES Statiblend® PA6/6 02013 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforAdditive: Impact ModifierFeatures: Conductive and Impact ModifiedUL File Number: E157318TPCI# 1039101Informati.. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP VERTON MV008S PP (Asia Pacific) LNP VERTON* MV008S is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ASTM D792 |
Washington Penn Homopolymer Polypropylene 40% Talc Filled Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi.. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ISO 1183 |
Tisan TISLAMID® 66 15% Glass Fiber Reinforced Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ISO 1183 |
Wolf Kunststoff ZEDEX® ZX-100EL63 A1G Polymer Alloy, Elastomer Modified Main Characteristics: Rubbery; Soft; High shock absorption; High impact resistance; Elongation > 300%Applications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automitve Technol.. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | Cured |
Hexcel® HexPly® 913 125°C Curing Epoxy Matrix HexPly® 913 is a proven modified epoxy matrix with a low temperature cure cycle which exhibits outstanding environmental resistance, whilst retaining good hot/wet mechanical performance. This versa.. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | |
Trelleborg Emerson & Cuming Stycast® W-66/17M-1 Two-Component Epoxy High Service Temp Encapsulant Features and Typical ApplicationsAbility to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in har.. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ISO 1183 |
DuPont Performance Polymers Hytrel® DYM1300 BK320 TPC-ET
(Unverified Data**) Hytrel® DYM1300 is a high performance thermoplastic elastomer with high modulus, suited for air bag door applications.Information provided by DuPont Performance Polymers |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | |
DuPont Performance Polymers Neoprene TW-100 Polychloroprene Rubber Neoprene Type TW-100 is a polychloroprene homopolymer, has excellent polymer stability, and a fast crystallization rate. Physical form: Chips. Color: Silver Gray to light amber. Distinguishing Fe.. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | |
DuPont Performance Polymers Neoprene WB Polychloroprene Rubber Neoprene Type WB is a polychloroprene homopolymer, has excellent polymer stability, and a medium crystallization rate. Physical form: Chips. Color: White to Silver Gray. Distinguishing Features: .. |
|||
Density | 1.23 - 1.27 g/cc | 0.0444 - 0.0459 lb/in³ | ISO R 1183 |
Fainplast Compounds CKL 70 Flexible PVC, Sheathing Lead Free General purposes |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® 70G13HS1L NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G13HS1L NC010 is a 13% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor.. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ISO 1183/A |
Addiplast Addilene H 520 T40 Polypropylene Homopolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ISO 1183 |
Akro-Plastic Akromid® B3 GF 15 (2469) PA 6 Conditioned, 15% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | dry; ISO 1183 |
BASF Ultramid® 1403-2 BK ND3007 PA66 (Conditioned) |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | dry; ISO 1183 |
BASF Ultramid® 8231G HS BK-102 14% Glass Filled PA6 (Conditioned) Ultramid 8231G HS BK-102 is a black pigmented heat stabilized, 14% glass fiber reinforced PA6 injection molding compound.The glass fiber reinforcement enhances performance such as strength, stiffnes.. |
|||
Density | 1.23 - 1.27 g/cc | 0.0444 - 0.0459 lb/in³ | ISO R 1184 |
Fainplast Compounds MPH 85 Medical Flexible PVC, Extrusion Tubolar apparatus |
|||
Density | 1.23 - 1.27 g/cc | 0.0444 - 0.0459 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 6316/AM Flexible PVC, Lead Free Anti-mould profiles |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | Polymer |
DuPont Performance Polymers Neoprene 571 Polychloroprene
(discontinued **) Main feature: High tensile strength. Principal uses include: Dipped goods, Elasticized concrete, Adhesives (Cord) Coatings.Solids content: 50%. Initial pH: 12. Surface tension: 40 dyne/cm. Polym.. |
|||
Density | 1.23 g/cc | 0.0444 lb/in³ | ISO 1183 |
Polykemi AB POLYfill PPH T5040 FC VT Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Density | 1.23 - 1.27 g/cc | 0.0444 - 0.0459 lb/in³ | ISO R 1183 |
Fainplast Compounds PMP 57 Flexible PVC, Extrusion Modified with PU Profiles mixed rubber/PU |