Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.00 GPa | 870 ksi | ASTM D638 |
NCMT NanoPAC™ G3000 High Performance Polypropylene Nanocomposite Applications: Automobile Construction MaterialInformation provided by Nano Composite Materials Technology Limited |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527 |
Nilit FRIANYL A63 W-GV15 Nylon 6.6 for injection molding, 15% glass fiber reinforced Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527 |
Nilit FRIANYL B63 SG-GV 2010 Nylon 6 for injection molding, 20% mineral filled and 10% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527-1/-2 |
Lanxess Pocan® TP 740-101 000000 PBT + ASA, 15% Glass Fiber PBT+ASA, 15% glass fibers, injection molding, low tendency to warp, improved surface finish |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527-1/-2 |
Lanxess Durethan® BM 240 H2.0 901510 Nylon 6, 40% Mineral PA 6, injection molding grade, 40% mineral, isotopic properties, good heat-ageing resistance |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | |
LATI Latilub 66-01M G/15 PA66, 15% Glass Fiber Reinforced, Molybdenum disulphide Filled Self-lubricating product based on Polyamide 66 (PA66). Molybdenum disulphide. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | 1 mm/min; ISO 527-1 |
Sax Polymers SAXAMID 226F3 Nylon 6.6, 15% Glass Fiber SAXAMID 226F3 is a polyamide 6.6 injection-molding-grade reinforced with 15% glass fibers. This grade is suitable for applications requiring high strength and very good flow properties during proces.. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527 |
Polyram PlusTek PA351M8 Nylon 6.6 for Injection Molding, 40% Mineral Reinforced 40% Minerals Reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527 |
Polyram PlusTek PD304G6YL55 Nylon 12 for Injection Molding, 30% Glass-fiber Reinforced 30% Glass-fiber reinforced Nylon 12 for injection molding applications. UL listed.Information provided by Polyram. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | |
Covestro Bayblend® T 88-4N Polycarbonate/ABS Blend, 20% Glass Fiber Contains 20% glass fiber reinforcement, high stiffness.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – .. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | |
Covestro Makrolon® 9125 Polycarbonate Medium viscosity, flame retardant extrusion and injection molding grade with 20% standard glass fibers and easy mold release agent.Information provided by Bayer.As of 1 September 2015, Bayer Materia.. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | cond; ISO 527-1/-2 |
DSM Novamid® 1015G33-8 NAT PA6-GF33 33% Glass Reinforced, Injection Molding |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® BG-30 S PA6-GF30 Product description: Grilon BG-30 S is a heat stabilized PA6 injection molding grade with 30% glass fibers. Grilon BG-30 S has the following important properties: Excellent surface finishEasy flowin.. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® BG-30/2 PA6-GF30 Product description: Grilon BG-30/2 is a heat stabilized, normal viscosity PA6 injection molding grade with 30% glass fibers. Grilon BG-30/2 has the following important properties: High stiffnessGoo.. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527-1/-2 |
DSM Stanyl® 46HF4130 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527-1/-2 |
DSM Stanyl® TW200F6 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized (North America) Information provided by DSM Engineering Plastics. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527-1/-2 |
DSM Stanyl® TW275F6 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized, Molydisulfide Lubricated (North America) Information provided by DSM Engineering Plastics. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600 MRGV 20/20 HWCP 20% Mineral and 20% Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600 MZ 315 CP Combination Nylon 66, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® LV-30H FWA nat PA12-GF30 Product description: Grilamid LV-30H FWA natural is a 30 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: Stiffness combined with h.. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSM-30/2 PA666-MD30 Product description: Grilon TSM-30/2 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% mineral filler. Grilon TSM-30/2 has the following important properties: Excell.. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 74G33J NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Polyamide 66 + Polyamide 6 Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527 |
Eurotec® Tecomid® NB40 KK30 NL PA 6 30% glass fiber/mineral reinforced, low warpage Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® A3 GF 25 (2420) PA 6.6 Conditioned, 25% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | 1mm/min; ISO 527 |
BASF Ultradur B 4300 G3 15% Glass Filled PBT Ultradur B 4300 G3 is an easy flowing injection molding PBT with 15% glass fiber reinforcement for rigid, tough, and dimensionally stable parts. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600 MR 409 HWCP 40% Mineral Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® 3412ECR PC (Asia Pacific) Lexan* 3412ECR Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V0 rating and is available in v.. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | 1mm/min; ISO 527 |
BASF Ultradur B 4040 G3 HT BK5830 15% Glass Filled PBT/PET Ultradur B 4040 G3 HT BK5830 is a 15% glass filled, pigmented black, injection molding PBT. It is a resin for molding household appliances and equipment which must be resistant to chemicals and oth.. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527 |
Polyram Polytron P30N07 Polypropylene, 30% Long Glass Fiber, UV Stabilized A chemically coupled 30% LGF reinforced natural PP, heat stabilized, UV stabilized for injection molding applications.Information provided by Polyram. |